DOWSIL 90-006 RF

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 90-006 RF

Main features

  • Two-Hour Working Time at 25 deg C
  • Mixing, Loading, Dispensing, and Assembly Processing
  • Prepared/Primed Aerospace-Material Adhesion

Product Description

DOWSIL™ 90-006 RF Sealant & Catalyst Kit is a two-part, high-viscosity silicone elastomer for aerospace sealing and bonding applications. The red base and green curing agent are mixed at a 10:1 ratio by weight, with contrasting colors providing a visual indication of mixing uniformity. The catalyzed material has a typical two-hour working time at 25°C and cures at room temperature. It adheres well to properly prepared and primed glass, cured silicone rubber, cork, phenolic, polyester, epoxy, silicone-resin laminates, stainless steel, titanium, aluminum, and other metals. After cure, the elastomer has a typical Shore A hardness of 48, tensile strength of 600 psi, and elongation at break of 130%.

Key features

  • Two-part room-temperature cure: The base and curing agent are combined at a 10:1 ratio by weight before application.
  • Two-hour working time: The catalyzed material remains usable for a minimum of two hours at 25°C unless otherwise specified.
  • Visual mixing confirmation: Contrasting red and green components indicate uniform blending when a consistent color is achieved.
  • High-viscosity base: Typical base viscosity is 1,200,000 mPa·s at 25°C.
  • Primed-substrate adhesion: Suitable substrates include glass, silicone rubber, laminates, stainless steel, titanium, aluminum, and other metals when properly prepared.

Applications / Suitable for

  • Sealing and bonding aerospace components and assemblies
  • Primed metal assemblies using stainless steel, titanium, aluminum, and other metals
  • Assemblies incorporating glass, cured silicone rubber, cork, phenolic, polyester, epoxy, or silicone-resin laminates

Technical Specifications

General Properties
Color
The color
Red (Base) / Green (Curing Agent)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,200,000 mPa.s

Additional Information

Aerospace silicone sealants

DOWSIL™ 90-006 RF Sealant & Catalyst Kit

A two-part, high-viscosity silicone elastomer for aerospace sealing and bonding. The red base and green curing agent are mixed at 10:1 by weight, remain usable for a minimum of two hours at 25°C, and cure at room temperature to form a firm elastomer that adheres well to properly prepared and primed surfaces.

Two-part silicone elastomer 10:1 mix ratio by weight Two-hour working time Room-temperature cure Red and green components
DOWSIL 90-006 RF Sealant and Catalyst Kit showing the two-component aerospace silicone packaging

Two-component DOWSIL™ 90-006 RF Sealant & Catalyst Kit for controlled proportioning, mixing, and application.

Before mixing and cure

As-supplied and catalyzed properties

Typical values are provided for product evaluation and are not intended for use as guaranteed specifications. Catalyzed values are based on a 10:1 base-to-curing-agent ratio by weight.

Property Value Unit Condition or context
Product form Two-part, high-viscosity silicone elastomer — Base and separate curing agent
Component colors Red / green — Base / curing agent; uniform color indicates uniform blending
Base viscosity 1,200,000 mPa·s CTM 0050 / ASTM D1084 at 25°C
Mixing ratio 10:1 By weight Base to curing agent
Working time 2 hours Typical at 25°C after catalyst addition
Tack-free time 2 hours CTM 0095; surface-cure timing is distinct from complete cure
Extrusion rate 200 g/min CTM 0364; tested two hours after mixing
Processing

Surface preparation, mixing, and application

Prepare the bonding surfaces before combining the components. Add one part curing agent to ten parts base by weight and mix until the contrasting colors form a uniform blend. Apply the catalyzed sealant by spatula or load it into a cartridge for pressure-gun dispensing.

Surface preparation: Clean with the specified solvent and a slightly abrasive pad or coarse lint-free cloth, rinse with acetone or methyl ethyl ketone, and allow the surface to dry before priming.
Primer: Apply a thin coat of DOWSIL™ PR-1200 RTV Prime Coat to prepared metal or plastic surfaces and allow it to dry for at least one hour, subject to relative humidity.
Mixing: Combine the base and curing agent at 10:1 by weight. Mix by hand for 2–5 minutes or for approximately 40 cycles in a mechanical mixer until the color is uniform.
Application window: The catalyzed material is usable for a minimum of two hours at 25°C unless otherwise specified.

 

Storage and handling

Store the unopened kit at or below 32°C. Under these conditions, the product has a usable life of 12 months from the date of production. The sealant and catalyst are available together in 453 g, 5 kg, 27.9 kg, and 199.5 kg kits.

After cure

Cured properties

Typical physical-property values are based on material cured at 25°C and 50% relative humidity. They are not intended as guaranteed specifications or assembly-level performance limits.

Property Typical value Unit or condition
Durometer hardness 48 Shore A; CTM 0099 / ASTM D2240; 48-hour value
Tensile strength 600 psi; CTM 0137A / ASTM D412
Elongation at break 130 %; CTM 0137A / ASTM D412
Peel strength 5.00 ppi; cohesive failure
Product resources

Aerospace and transportation selection guides

These Dow guides provide broader context for evaluating silicone materials in spacecraft, satellite, and transportation-system bonding and sealing applications.

SELECTION guide
Silicones for spaceship and satellite applications
Reviews Dow silicone technologies and material-selection considerations for spacecraft and satellite systems, including aerospace bonding, sealing, protection, and assembly contexts.
View spaceship and satellite silicone guide
selection guide
Adhesive and sealant solutions for vehicle-system design
Provides broader selection guidance for Dow adhesive and sealant technologies used in transportation assemblies and component systems.
View vehicle-system selection guide
Technical support

Evaluate DOWSIL™ 90-006 RF for your aerospace assembly

Contact Krayden for support reviewing substrate preparation, primer selection, weighing and mixing controls, working-time requirements, application equipment, packaging options, and cured-property considerations for your aerospace sealing or bonding process.