DOWSIL 9-1374

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 9-1374

Main features

  • One-Part Low-Odor Neutral Cure
  • Primerless Multi-Substrate Adhesion
  • -55 to 180 deg C Flexibility

Product Description

DOWSIL™ 9-1374 Silicone Sealant is a one-part, 100% silicone adhesive-sealant supplied as a clear, non-slump paste. Its alkoxy neutral-cure system reacts with atmospheric moisture at room temperature to form a tough, flexible silicone rubber with low odor. The product provides good unprimed adhesion to many commonly used substrates, including wood, steel, aluminum, paints, and certain plastics. It is suited to flexible bonding between materials with different thermal expansion rates, including glass-to-metal, glass-to-plastic, and metal-to-plastic assemblies. The sealant is also used for formed-in-place gaskets and environmental sealing or protection of parts and substrates. Once cured, it remains stable and flexible from -55°C to 180°C (-67°F to 356°F).

Key features

  • Neutral moisture cure: The one-part alkoxy silicone cures at room temperature with low odor and requires no component mixing.
  • Flexible multi-substrate bonding: Good unprimed adhesion to many common materials supports assemblies combining substrates with different thermal expansion rates.
  • Broad temperature range: The cured silicone remains stable and flexible from -55°C to 180°C (-67°F to 356°F).

Applications / Suitable for

  • Flexible bonding of glass, metals, plastics, wood, and painted surfaces where supported by substrate testing
  • Formed-in-place gaskets
  • Environmental sealing and protection of parts and substrates
Product Family

DOWSIL 9-1374

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Non-slump paste
Color
The color
Clear
Physical Properties
Tack-Free Time
40 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
300–550 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the sealant as supplied and during initial room-temperature moisture cure. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance Non-slump paste — As supplied; typical
Color Clear — As supplied; typical
Extrusion rate 340 g/minute CTM 0364 / ASTM D2452; 1/8 in (3.18 mm) nozzle at 90 psi (0.62 MPa)
Skin-over time 5 minutes CTM 0098; typical
Tack-free time 40 minutes CTM 0095; time to develop a non-tacky surface based on adhesion to polyethylene film

After-processing / final-state properties

Typical mechanical properties after curing for seven days in air at 23°C (73°F) and 50% relative humidity. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Durometer hardness 21 Shore A points ASTM C661; cured 7 days at 23°C (73°F) and 50% RH
Tensile strength 237 psi CTM 0137A / ASTM D412; cured 7 days at 23°C (73°F) and 50% RH
Elongation 401 % CTM 0137A / ASTM D412; cured 7 days at 23°C (73°F) and 50% RH
Modulus at 100% elongation 64 psi CTM 0137A / ASTM D412; cured 7 days at 23°C (73°F) and 50% RH
Elongation at break 300–550 % CTM 0137A / ASTM D412; cured 7 days at 23°C (73°F) and 50% RH
Stable and flexible temperature range -55 to 180
(-67 to 356)
°C
(°F)
Cured silicone; documented stability and flexibility range