DOWSIL 838

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 838

Main features

  • One-Part Moisture-Cure Application
  • Non-Sag Placement Control
  • Flexible Cured Material

Product Description

DOWSIL™ 838 Silicone Adhesive Sealant is a one-part, white, non-flowing silicone adhesive for general-purpose bonding, sealing, and component stabilization in electronic assemblies. The moisture-cure material requires no mixing and cures at room temperature, with mild heat below 60°C (140°F) available to accelerate cure. Its non-flowing consistency supports automated or manual needle dispensing, while the cured elastomer combines a Shore A hardness of 31 with a tensile modulus of 0.4 MPa for flexible attachment and sealing. Applications include sealing openings in modules and housings, stabilizing individual components, assembling components on printed wiring boards, sealing around wired and electrical leads, and yoke assembly.

Key features

  • One-part room-temperature cure: Requires no mixing or curing oven under standard moisture-cure conditions.
  • Non-flowing dispense behavior: Supports controlled application through automated or manual needle dispensing systems.
  • Flexible cured silicone: Provides a typical Shore A hardness of 31 and tensile modulus of 0.4 MPa, with a UL 94 HB flammability classification.

Applications / Suitable for

  • Sealing openings in electronic modules and housings
  • Adding mechanical stability to individual components
  • Assembly of components on printed wiring boards
  • Sealing around wired and electrical leads
  • Yoke assembly

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.02
Physical Properties
Tack-Free Time
46 minutes
Thermal Properties
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
94 HB

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Product form One-part, non-flowing adhesive — As supplied
Color White — As supplied
Extrusion rate 199.2 g/min Typical value
Flow rate – slump 0 in / 0.1 cm — Typical value

After-processing / final-state properties

Typical cured-material values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific gravity 1.02 — Cured material; typical value
Tensile strength 270 / 1.9 / 19 psi / MPa / kg/cm² Cured material; typical value
Tensile modulus 60 / 0.4 / 4 psi / MPa / kg/cm² Cured material; typical value
Durometer hardness 31 Shore A Cured material; typical value
UL flammability classification 94 HB — UL flammability classification
Useful temperature range -45 to 200 °C For most long-term uses; application performance should be verified at temperature extremes