DOWSIL 832

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 832

Main features

  • Primerless Multi-Substrate Adhesion
  • One-Part Low-Odor Neutral Cure
  • -55 to 149 deg C Service

Product Description

DOWSIL™ 832 Multi-Surface Adhesive Sealant is a one-component, ready-to-use, 100% silicone RTV for bonding, sealing, assembly, and maintenance applications. The nonslumping paste cures through atmospheric moisture using a low-odor, neutral alcohol cure that is noncorrosive to metals and other corrosion-sensitive materials. It provides unprimed adhesion to many common substrates, including glass, metals, masonry, concrete, rubber, ABS, PVC, and polycarbonate. The cured material forms a flexible silicone rubber seal with a typical Shore A hardness of 35, tensile strength of 350 psi, and elongation of 420%. Applications include roof penetrations, gutters, concrete floor seams, marine equipment and windows, pipes, threaded connections, and original equipment assembly.

Key features

  • Broad substrate adhesion: Provides superior unprimed adhesion to a wide variety of glass, metal, masonry, concrete, rubber, and plastic surfaces.
  • Neutral, noncorrosive cure: The low-odor alcohol-cure system is suitable for use with metals and other corrosion-sensitive materials.
  • Flexible cured silicone: Delivers 420% typical elongation and a continuous use-temperature range from -55 to 149°C.

Applications / Suitable for

  • Sealing and repairing roof penetrations, gutters, and concrete floor seams
  • Marine equipment, windows, pipes, and threaded connections
  • Bonding, sealing, and assembly of original equipment components

Technical Specifications

Physical Properties
Tack-Free Time
50–90 minutes
General Properties
Color
The color
Off-white, black, gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.33
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
420 %

Additional Information

Silicone adhesive sealants

DOWSIL™ 832 Multi-Surface Adhesive Sealant

A one-component, ready-to-use silicone RTV for bonding, sealing, assembly, and maintenance. The low-odor, neutral alcohol cure is noncorrosive to metals, while superior unprimed adhesion supports application to glass, metals, masonry, concrete, rubber, ABS, PVC, polycarbonate, and other common substrates.

One-component RTV 100% silicone Neutral alcohol cure Noncorrosive Nonslumping paste Low odor
DOWSIL 832 Multi-Surface Adhesive Sealant product packaging

One-component DOWSIL™ 832 Multi-Surface Adhesive Sealant for industrial assembly, sealing, and maintenance.

Before cure

As-supplied properties

Typical values are provided for product evaluation and are not intended for use as guaranteed specifications. Cure-related values are measured at 25°C and 50% relative humidity.

Property Value Unit Condition or context
Consistency Nonslumping paste — One-component, ready-to-use material
Corrosion properties Noncorrosive — Neutral alcohol cure
Extrusion rate 133 g/min CTM 0364; 1/8-inch nozzle at 90 psi
Viscosity 496 Pa·s CTM 1377; low shear at 1 s-1
Viscosity 172 Pa·s CTM 1377; high shear at 10 s-1
Skin-over time 20 minutes CTM 0098; 25°C and 50% relative humidity
Tack-free time 50–90 minutes CTM 0095; 25°C and 50% relative humidity
Specific gravity 1.33 — CTM 0022 at 25°C
Processing

Application and cure

Apply DOWSIL™ 832 to clean, dry, frost-free surfaces. The ready-to-use material requires no mixing and cures through reaction with moisture in the air. Primer is typically unnecessary, although DOWSIL™ 1205 PR-Prime Coat is recommended for best adhesion to concrete.

Surface preparation: Surfaces must be clean, dry, frost-free, and free from oil and dirt.
Primer: Primer is generally not required; use DOWSIL™ 1205 PR-Prime Coat for best adhesion to concrete.
Surface-cure timing: Typical skin-over time is 20 minutes and tack-free time is 50–90 minutes at 25°C and 50% relative humidity.
DOWSIL 832 adhesive sealant being dispensed as a controlled bead onto a clean assembly surface

 

Storage and Handling

Store at or below 32°C. Under these conditions, the product has a usable life of 18 months from its date of manufacture. For best results, use the material completely within six months after opening and keep the container sealed when not in use. A cured plug may form in the dispensing tip during storage; it can be removed without affecting the remaining material.

After cure

Cured properties

Typical laboratory values after seven days of cure at 25°C and 50% relative humidity. These values are not intended for use as guaranteed specifications or universal joint-performance limits.

Property Typical value Unit or condition
Color Off-white, black, gray Selected colors
Durometer hardness 35 Shore A; CTM 0099
Tensile strength 350 psi; CTM 0137A
Elongation 420 %; CTM 0137A
Peel strength — ABS >35 ppi; CTM 0293
Peel strength — polycarbonate, unprimed >35 ppi; CTM 0293
Peel strength — PVC >30 ppi; CTM 0293
Peel strength — milled aluminum >35 ppi; CTM 0293
Peel strength — carbon steel >35 ppi; CTM 0293
Peel strength — copper >35 ppi; CTM 0293
Peel strength — glass >30 ppi; CTM 0293
Continuous use temperature -55 to 149 °C (-67 to 300°F)
Intermittent use temperature 177 °C (350°F)
Applications

Bonding, sealing, and maintenance applications

DOWSIL™ 832 is used where broad adhesion or a noncorrosive silicone sealant is required for repair, maintenance, sealing, or component assembly.

Silicone sealant applied around a roof penetration and gutter joint
Building repair and maintenance
Applications include sealing and repairing roof penetrations, gutters, and concrete floor seams. Use DOWSIL™ 1205 PR-Prime Coat where best adhesion to concrete is required.
Silicone adhesive sealant applied around a marine equipment window
Marine equipment and windows
The noncorrosive silicone formulation is used for sealing marine equipment and windows where adhesion to glass, metals, rubber, or plastics may be required.
DOWSIL 832 silicone adhesive sealant used in an original equipment component assembly
Equipment and component assembly
Suitable for bonding, sealing, and assembling original equipment components, as well as sealing pipes and threaded connections where the documented product limitations are acceptable.

Product resources

Silicones for spaceship and satellite applications
Review Dow silicone technologies and product-selection considerations for spacecraft and satellite applications.
View resource
Adhesive and sealant solutions for vehicle-system design
Explore Dow adhesive and sealant selection guidance for bonding and sealing components across vehicle systems.
View resource
Silicone sealants and foams for industrial, appliance, and maintenance applications
Compare Dow silicone sealant and foam technologies for industrial equipment, appliances, assembly, and maintenance.
View resource
Next steps

Evaluate DOWSIL™ 832 for your application

Contact Krayden for support evaluating substrate adhesion, surface preparation, primer requirements, application conditions, packaging options, joint limitations, and service-temperature requirements for your bonding, sealing, assembly, or maintenance process.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers