DOWSIL 791

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

DOWSIL 791

Main features

  • +/-50% Weatherseal Movement
  • Zero-Flow Weatherseal Application
  • 20-Minute Weatherseal Tooling

Product Description

DOWSIL 791 Silicone Weatherproofing Sealant is a one-part, neutral-cure silicone sealant for weathersealing expansion, connection, perimeter and other movement joints in curtain walls and building facades. The ready-to-use material has zero measured flow, a 140 g/min extrusion rate and a 20-minute working time at 23 deg C and 50% relative humidity. After 21 days at 25 deg C and 50% relative humidity, the sealant reaches Shore A 34 hardness, 30 lb/in peel strength and +/- 50% joint movement capability. It is intended for general glazing and weatherseal joints and is not specified for structural glazing.

Key features

  • Zero-flow weatherseal application: ASTM C639 flow is 0 at 23 deg C and 50% relative humidity.
  • 20-minute working time: Supports placement and tooling before skin formation.
  • +/- 50% joint movement: ASTM C719 movement capability applies after 21 days of cure.

Applications

Weathersealing expansion, connection, perimeter and movement joints in curtain walls and building facades.

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.50
Physical Properties
Extrusion Rate
220 g/min
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
700 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and cure-development properties tested at 23 deg C and 50% relative humidity unless noted.

Property Value Unit Method / condition
Flow, sag or slump 0 in ASTM C639
Extrusion rate 140 g/min ASTM C603
Working time 20 min At 23 deg C and 50% RH
Tack-free time 40 min ASTM C679; 25 deg C and 50% RH
Curing time 7-14 days At 25 deg C and 50% RH
VOC content 31 g/L SCAQMD basis
Technical properties

After-processing / final-state properties

Typical properties after 21 days at 25 deg C and 50% relative humidity.

Property Value Unit Method / condition
Durometer hardness 34 Shore A ASTM D2240
Peel strength 30 (5.4) lb/in (kg/cm) ASTM C794
Joint movement capability +/- 50 % ASTM C719
Tensile adhesion at 25% extension 40 (0.276) psi (MPa) ASTM C1135
Tensile adhesion at 50% extension 60 (0.) psi (MPa) ASTM C1135