DOWSIL 786

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 786

Main features

  • Mildew-Resistant High-Humidity Sanitary Sealant
  • Permanently Flexible Cured Seal
  • One-Part Non-Sag Application

Product Description

DOWSIL™ 786 Silicone Sealant is a one-part, ready-to-use, acetoxy-cure silicone rubber sealant for sealing nonporous surfaces in sanitary and plumbing applications. It contains an antimicrobial, and the cured sealant is mildew resistant, permanently flexible, and resistant to staining, spotting, and color changes. The non-sag material adheres to many surfaces, including porcelain, cultured marble, painted areas, and glass, although adhesion and compatibility should be evaluated for each application. It is available in white, translucent white, and clear.

Key features

  • Mildew-resistant cured sealant: Contains an antimicrobial and is formulated for sanitary areas exposed to high humidity.
  • Permanent flexibility: Remains flexible without shrinking, cracking, crumbling, or drying out.
  • Ready-to-use, non-sag application: The one-part sealant can be applied directly from a cartridge and shows no flow, sag, or slump under ASTM C 639.

Applications / Suitable for

  • Sealing around shower and tub enclosures
  • Sealing around tubs, sinks, urinals, whirlpools, and bathroom fixtures
  • Waterproofing rimless sinks
  • Ceramic tile grouting
Product Family

DOWSIL 786

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Tack-Free Time
20 minutes
General Properties
Color
The color
White, translucent white, clear
Mechanical Properties
Peel Strength
3.5 kN/m

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ 786 Silicone Sealant before cure. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color White, translucent white, clear — ASTM C 639
Tack-free time 20 minutes ASTM C 679; 25°C (77°F), 50% RH
Tooling time 5–11 minutes Typical value
Flow, sag, or slump Nil — ASTM C 639
Extrusion rate 350 g/min ASTM C 603
Volatile organic content 22 g/L ASTM C 603; based on California SCAQMD
Shelf life 900 days Dow product-page typical property; store at or below 32°C (90°F) in the original unopened container

After-processing / final-state properties

Typical properties measured after seven days of cure at 25°C (77°F) and 50% relative humidity. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Durometer hardness 25 Shore A points ASTM D 2240; cured 7 days at 25°C (77°F), 50% RH
Ultimate tensile strength 325 (2.1) psi (MPa) ASTM D 412; cured 7 days at 25°C (77°F), 50% RH
Tear strength 25 (4.4) ppi (kN/m) ASTM D 624; cured 7 days at 25°C (77°F), 50% RH
Peel strength 20 (3.5) pli (kN/m) ASTM C 794; cured 7 days at 25°C (77°F), 50% RH