DOWSIL 7500

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL 7500

Main features

  • Color-Coded 1:1 Mixing
  • Five-Minute 125 deg C Cure
  • Stencil-Printable Electronics Bonding

Product Description

DOWSIL 7500 Adhesive Kit uses color-coded two-part components and a 1:1 mix ratio to create a translucent green, heat-cure silicone pressure-sensitive adhesive for electronics assembly. Part A is translucent yellow and Part B is translucent blue, helping confirm component loading and mixing. The material is stencil- or screen-printable and cures in five minutes at 125 deg C to a soft pressure-sensitive elastomer for bonding electronic components, FR4, heat sinks and module parts. Complex-viscosity values at defined shear rates and a thixotropic ratio of 2.3 support process evaluation, while the cured adhesive has Shore 00 hardness and 90-degree peel data.

Key features

  • Color-coded 1:1 mixing: Yellow and blue components produce a green mixed adhesive for visual verification.
  • Five-minute heat cure: Typical cure time is five minutes at 125 deg C.
  • Stencil and screen printability: Rheology supports patterned electronics-assembly application.

Applications

Pressure-sensitive bonding of electronic components, FR4, heat sinks and module components.

Product Family

DOWSIL 7500

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent yellow / Translucent blue
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (A /B)
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
2.3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material and process values. Values are not specifications.

Property Value Unit Method / condition
Mix ratio 1:1 Part A to Part B
Component appearance Translucent yellow / translucent blue Part A / Part B
Mixed appearance Translucent green After correct mixing
Part A / Part B complex viscosity 100000 / 80000 cP CTM1098; 10 rad/sec
Mixed complex viscosity 81000 / 35500 cP CTM1098; 10 / 100 rad/sec
Thixotropic ratio 2.3 CTM1098
Heat-cure time 5 min At 125 deg C
Shelf life 12 months At 25 deg C
Technical properties

After-processing / final-state properties

Typical properties of the heat-cured pressure-sensitive adhesive. Cure condition is five minutes at 125 deg C unless otherwise stated.

Property Value Unit Method / condition
Cured form Soft pressure-sensitive elastomer Heat-cured mixed adhesive
Durometer hardness 40 Shore 00 CTM0099
90-degree peel adhesion 2.4 lb/in CTM0270