DOWSIL 748

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 748

Main features

  • Non-Corrosive Application Formulation
  • 15-Minute Tack-Free Time
  • 55 to 177 deg C Service Range

Product Description

DOWSIL™ 748 Non-Corrosive Sealant is a one-component, ready-to-use, non-slump silicone adhesive and sealant that moisture-cures at room temperature to form a tough, rubbery solid. Its alkoxy cure mechanism produces no corrosive by-products, supporting bonding and sealing around copper, electrical equipment, printed circuit board assemblies, and other corrosion-sensitive components. The off-white material develops a skin in approximately 15 minutes and becomes tack-free in less than 30 minutes at 25°C and 50% relative humidity. Once cured, it provides a Shore A hardness of 35, 350% elongation, electrical-insulation properties, and service capability from -55 to 177°C for extended periods, with shorter exposure up to 204°C.

Key features

  • Non-corrosive alkoxy cure: Produces no corrosive cure by-products and is suitable for use around copper and other corrosion-sensitive metals.
  • One-component, non-slump paste: Ready to apply without mixing, heating, or solvent-handling steps.
  • Electrical properties: Typical dielectric strength of 475 V/mil and volume resistivity of 7.7 × 1014 ohm·cm after cure.
  • Broad service-temperature capability: Suitable for extended exposure from -55 to 177°C and shorter exposure up to 204°C.
  • Environmental resistance: Cured silicone resists moisture, ozone, corona, and weathering.
  • Documented regulatory status: UL recognized and compliant with 21 CFR 177.2600 requirements when fully cured, washed, and used within applicable extractives limitations.

Applications / Suitable for

  • Bonding and sealing electrical equipment and printed circuit board system assemblies
  • Power and control connections, motors, junction boxes, control panels, and instrument assemblies
  • General-purpose industrial bonding and sealing where low odor and non-corrosive cure are required
  • Food-processing equipment applications requiring an appropriately cured and washed silicone material

Technical Specifications

Physical Properties
Tack-Free Time
30 minutes
General Properties
Color
The color
Off-white
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.33
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
350 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
1.63 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
7.7E14 Ohms⋅cm

Additional Information

Silicone sealants

DOWSIL™ 748 Non-Corrosive Sealant

A one-component, non-slump alkoxy silicone adhesive and sealant for general industrial and corrosion-sensitive electrical assemblies. The material cures with atmospheric moisture to form a tough rubber and combines non-corrosive cure chemistry with documented electrical properties, environmental resistance, and broad service-temperature capability.

One-component RTV Non-corrosive alkoxy cure Non-slump paste 15-minute skin-over Off-white
Material and working properties

As-supplied properties

Typical values measured at 25°C and 50% relative humidity unless otherwise stated. These values are not intended for specification writing.

Property Value Unit Method or condition
Consistency Non-slump paste — As supplied
Extrusion rate 150 g/min 1/8-inch nozzle at 90 psi
Skin-over time 15 min At 25°C and 50% relative humidity
Tack-free time 30 min At 25°C and 50% relative humidity
Cure time 36 hours 1/8-inch section at 25°C and 50% relative humidity
Full cure 7 days 1/8-inch section at 25°C and 50% relative humidity
Corrosion properties Non-corrosive — Alkoxy cure mechanism produces no corrosive cure by-products
Processing

Application and moisture cure

Apply the sealant to clean, prepared surfaces in a uniform layer. Cure progresses inward from surfaces exposed to atmospheric moisture, so joint thickness, exposed area, humidity, and substrate permeability affect the time required to reach the final cured state.

Surface preparation: Use clean surfaces. The sealant bonds to many metals, glass, silicone and organic resins, and vulcanized silicone rubber. Some plastics, including acrylic, may require DOWSIL™ 1205 Prime Coat.
Application and assembly: Apply to one surface and establish uniform contact before joining the second surface. Use enough pressure to displace the material and form contact across the bond area. A 15-mil glue line is recommended for best adhesion.
Tooling and cure: Complete tooling before the surface skins, approximately 15 minutes at room temperature and 50% relative humidity. Cure requires at least 20% relative humidity; lower humidity or large enclosed bond areas extend cure time.
Cure depth: At room temperature and approximately 50% relative humidity, the sealant cures about 75 mils in 24 hours and approximately 1/4 inch in 72 hours. Sections 1/2 inch deep may require up to two weeks for complete cure.
Storage and handling

Store at or below 32°C in tightly sealed containers. Shelf life is 24 months from the date of manufacture when stored under the stated conditions. Because the material reacts with atmospheric moisture, reseal opened containers promptly. A cured plug may form in a tube tip during storage and can be removed without affecting the remaining material.

Final material state

Cured physical and electrical properties

Typical cured values after seven days at 25°C and 50% relative humidity unless otherwise stated. Values are not intended for specification writing.

Property Value Unit Method or condition
Physical form Tough, rubbery solid — After cure
Color Off-white — Cured material
Specific gravity 1.33 — At 25°C
Peel strength 25 (4.4) ppi (kN/m) 1/4-inch steel strip bonded to aluminum
Durometer hardness 35 Shore A ASTM D2240
Tensile strength 275 psi ASTM D412
Elongation 350 % ASTM D412 tensile specimen property
Dielectric strength 475 V/mil ASTM D149
Volume resistivity 7.7 × 1014 ohm·cm ASTM D257
Dielectric constant 3.30 at 100 Hz
3.21 at 10 kHz
— ASTM D150 at 25°C
Dissipation factor 8.7 × 10-3 at 100 Hz
2.8 × 10-3 at 10 kHz
— ASTM D150 at 25°C
Service temperature -55 to 177 extended
Up to 204 shorter exposure
°C Actual suitability depends on the specific application environment
UL status Recognized to 105°C where elongation is not essential; UL 94 HB — UL File E40195 (N)
FDA status Meets 21 CFR 177.2600 requirements when fully cured and washed — Subject to end-user compliance with applicable total extractives limitations
 

Product resources

DOWSIL™ Silicone Sealants and Foams for Industrial, Appliance and Maintenance
A selection guide comparing industrial silicone sealant technologies, cure types, application areas, service-temperature ranges, physical properties, listings, and substrate-adhesion guidance. It includes product-specific selection information for DOWSIL™ 748.
View resource
Certified Solutions for Food and Beverage Processing
Supporting information for evaluating silicone solutions used in food- and beverage-processing environments, including certification and regulatory considerations relevant to selecting materials for equipment and processing applications.
View resource
Next steps

Evaluate DOWSIL™ 748 for your sealing application

Contact Krayden to discuss substrate preparation, bondline geometry, moisture-cure conditions, electrical requirements, regulatory considerations, packaging availability, or sample needs for DOWSIL™ 748 Non-Corrosive Sealant.

Leading Brands Trust in Our Products and Services