DOWSIL 737

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 737

Main features

  • One-Part Neutral-Cure Silicone
  • 3 to 6-Minute Skin-Over
  • Primerless Multi-Substrate Adhesion

Product Description

DOWSIL™ 737 Neutral Cure Sealant is a one-part, oxime-cure silicone rubber supplied as a non-slumping paste for industrial bonding, sealing, formed-in-place gasketing, assembly, installation, and maintenance operations. It cures at room temperature when exposed to atmospheric moisture and adheres without primer to many common plastics, metals, painted surfaces, glass, and rubbers. The sealant develops a skin in 3–6 minutes and becomes tack-free in approximately 14 minutes at 25°C and 50% relative humidity. After cure, it remains flexible across a stated service-temperature range of -65°C to 177°C and provides weather resistance for assemblies exposed to sunlight, rain, snow, and temperature extremes.

Key features

  • One-part neutral cure: Moisture-cure silicone paste requiring no component mixing.
  • Non-slumping application: Stays in place after dispensing without sagging or running from the applied surface.
  • Rapid surface cure: Typical skin-over time of 3–6 minutes and tack-free time of 14 minutes at 25°C and 50% relative humidity.
  • Primerless adhesion to many materials: Adheres to many plastics, metals, painted surfaces, glass, and rubbers, subject to application testing.
  • Flexible cured silicone: Typical elongation greater than 300% after seven days of cure at 25°C and 50% relative humidity.
  • Broad service-temperature range: Cured material remains flexible from -65°C to 177°C.

Applications / Suitable for

  • Industrial OEM bonding, sealing, assembly, and installation operations
  • Formed-in-place gasketing and maintenance sealing
  • Appliance assembly and refrigerator or freezer liner sealing
  • Plastic molding, trim, and decal attachment
  • Waterproofing electrical components and sealing coaxial connectors
  • Protection of instrumentation assemblies

Technical Specifications

General Properties
Color
The color
Translucent, white, black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1,04
Physical Properties
Tack-Free Time
14 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
300 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
1.48 kV/mm

Additional Information

Industrial silicone sealant

DOWSIL™ 737 Neutral Cure Sealant

A one-part, non-slumping oxime-cure silicone for industrial bonding, sealing, formed-in-place gasketing, assembly, installation, and maintenance. It cures upon exposure to atmospheric moisture, adheres without primer to many common substrates, and remains flexible over a stated cured service-temperature range of -65°C to 177°C.

One-part oxime cure Non-slumping paste 3–6 minute skin-over Primerless adhesion to many materials -65°C to 177°C flexibility
DOWSIL™ 737 Neutral Cure Sealant product packaging

DOWSIL™ 737 Neutral Cure Sealant

As supplied

As-supplied properties

Typical values are not intended for use in preparing specifications. Preserve the stated method and test conditions when comparing products or evaluating dispensing behavior.

Property Typical value Unit Method / condition
Color Translucent, white or black — As supplied
Flow, sag or slump Nil in CTM 0062
Specific gravity 1.04 — CTM 0097
Extrusion rate 395 g/min CTM 0364; 1/8 in orifice at 90 psi
Skin-over time 3–6 min CTM 0098; exposed to air at 25°C and 50% RH
Tack-free time 14 min 25°C and 50% RH
Processing

Application and cure

Apply the sealant to clean, dry surfaces in a continuous operation. Tool immediately after dispensing and before the surface skin forms. Atmospheric moisture is required for cure, so the material should not be used in totally confined spaces without moisture exposure.

Surface condition: Surfaces must be clean and dry. Clean metal and glass with a suitable solvent and an oil-free rag while following the solvent supplier’s safe-handling instructions.
Priming: Priming is not required for most glass, aluminum, steel, and other common substrates. Conduct a test placement before general use.
Tooling window: Tool with light pressure immediately after application and before the typical 3–6 minute skin-over period has elapsed.
Handling condition: The sealant typically cures to a handling condition in 24 hours when exposed to atmospheric moisture.
Illustration of continuous sealant application and immediate tooling on clean, dry industrial substrates

 

Recommended application sequence

Stage 1
Prepare the surfaces
Remove contamination and confirm that the bonding or sealing surfaces are clean and dry. Evaluate adhesion on the actual substrate before production use.
Stage 2
Dispense continuously
Apply a continuous bead to the required joint, interface, gasket path, or assembly area. The non-slumping paste is intended to remain where placed.
Stage 3
Tool and allow to cure
Tool immediately with light pressure to spread the sealant against the substrate. Maintain exposure to atmospheric moisture during cure and avoid totally confined cure conditions.
Storage and handling

Store at or below 32°C in the original unopened container. Uncured material may be removed from tools and nonporous surfaces with an appropriate solvent. On porous surfaces, allow excess material to cure and remove it mechanically. Review the current safety data and container label before handling.

After cure

Cured properties

Physical-property values are typical after seven days of cure at 25°C and 50% relative humidity unless otherwise stated. They are not guaranteed specifications.

Property Typical value Unit Method / condition
Durometer hardness 33 Shore A points CTM 0099; cured seven days at 25°C and 50% RH
Tensile strength >175 psi CTM 0137A; cured seven days at 25°C and 50% RH
Elongation >300 % CTM 0137A; cured seven days at 25°C and 50% RH
Typical adhesion, peel strength 20 ppi CTM 0293; adhesion has been demonstrated on multiple listed industrial substrates
Dielectric strength 344 V/mil Cured material
Flexible service-temperature range -65 to 177 °C Stated range over which the cured material remains flexible
Applications

Industrial bonding and sealing applications

Industrial appliance assembly showing a sealant bead used between appliance components

Appliance and OEM assembly

The sealant is designed for diverse OEM and assembly operations, including use as an alternative to mechanical fasteners on large and small appliances and for sealing refrigerator or freezer liners. Refrigerator and freezer liner use does not constitute FDA approval for food-contact applications.

Formed-in-place silicone gasket applied as a continuous bead around an industrial enclosure flange

Formed-in-place gasketing and maintenance

The non-slumping paste can be applied in continuous gasket paths and maintenance seals where the material must remain in position during application. Atmospheric moisture access is required, and the product is not recommended for totally confined spaces or continuous water immersion.

Electrical connector and instrumentation enclosure protected with an applied silicone sealant

Electrical and instrumentation protection

Documented uses include waterproofing electrical components, sealing coaxial connectors, and protecting instrumentation assemblies. Evaluate adhesion, cure access, electrical requirements, and the compatibility of sensitive metals or polycarbonate under the intended assembly conditions.

Product support

Evaluate DOWSIL™ 737 for your assembly or sealing process

Contact Krayden to discuss substrate adhesion, surface preparation, dispensing and tooling requirements, moisture access during cure, service-temperature needs, sensitive-material compatibility, or sample evaluation for your industrial assembly, gasketing, appliance, electrical, or maintenance application.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers