Main features

  • Up to 260 deg C Continuous Service
  • Non-Slumping Vertical/Overhead Application
  • Flexible High-Temperature Silicone Sealing

Product Description

DOWSIL™ 736 Heat Resistant Sealant is a one-part, nonslumping silicone paste for high-temperature bonding, sealing, gasketing, potting, encapsulating and protective-coating applications. Atmospheric moisture cures the material at room temperature to a flexible rubbery solid. It supports continuous operation from -65 to 260°C and intermittent exposure to 315°C. The red, ready-to-use sealant can be applied on sidewalls and overhead surfaces and is used around appliance heating elements, industrial ovens, moving oven belts, aerospace gaskets and bag filters on smoke stacks.

Key features

  • High-temperature service: Continuous operation to 260°C and intermittent exposure to 315°C.
  • Nonslumping application: Will not sag or run on sidewalls or overhead surfaces.
  • Ready-to-use moisture cure: One-part paste cures at room temperature when exposed to atmospheric moisture.
  • Flexible cured rubber: Typical Shore A hardness of 26 and elongation of 600% after 72 hours of cure.

Applications

Heating-element sealing and encapsulation, aerospace gasketing, moving oven belts, industrial ovens, smoke-stack bag filters and other high-temperature bonding, sealing, potting, encapsulating and protective-coating applications.

Technical Specifications

General Properties
Color
The color
Red
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.04
Physical Properties
Tack-Free Time
17 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
600 %

Additional Information

High-temperature silicone sealant

DOWSIL™ 736 Heat Resistant Sealant

A one-part, nonslumping silicone paste for bonding, sealing, gasketing, potting, encapsulating and protective-coating applications exposed to high temperatures. The material cures at room temperature through atmospheric moisture to form a flexible rubbery solid and supports continuous operation to 260°C with intermittent exposure to 315°C.

One-part silicone Nonslumping paste Room-temperature moisture cure Continuous service to 260°C Intermittent exposure to 315°C
DOWSIL 736 Heat Resistant Sealant in its commercial red silicone sealant packaging

DOWSIL™ 736 Heat Resistant Sealant is supplied as a red, ready-to-use silicone paste.

Before cure

As-supplied properties

Typical values are provided for product evaluation and are not intended as guaranteed specifications.

Property Value Unit Condition or context
Composition One-part silicone — Ready-to-use moisture-cure system
Color Red — As supplied
Flow or slump Nil — Nonslumping paste
Extrusion rate 390 g/min 3.18 mm orifice at 90 psi
Specific gravity 1.04 — Typical as-supplied value
Skin-over time 10 minutes Exposed to air at 25°C and 50% relative humidity
Tack-free time 17 minutes Exposed to air at 25°C and 50% relative humidity
Cure time 24 hours 3 mm thickness at 25°C and 50% relative humidity
Processing

Surface preparation, application and cure

DOWSIL™ 736 is supplied ready to use and flows from its container under pressure. Thoroughly clean and degrease applicable metal and plastic surfaces before application. Roughen rubber surfaces with sandpaper and wipe them with a suitable solvent. Apply the paste in a uniform thickness and complete tooling before skin formation begins.

Tooling window
Within 5 minutes
Complete tooling promptly after application and remove masking tape immediately.
Tack-free time
17 minutes
Typical surface-cure time at 25°C and 50% relative humidity.
3 mm cure
About 24 hours
Typical time to form a rubbery solid at 25°C and 50% relative humidity.
Technician dispensing and tooling DOWSIL 736 Heat Resistant Sealant into a cleaned high-temperature equipment joint

Apply the sealant to properly prepared surfaces in a uniform thickness and complete tooling before skin formation.

Cure, priming and storage considerations

Atmospheric moisture is required for cure. Lower humidity, thicker sections and partial confinement extend cure time, while absolute confinement may prevent complete cure. For stronger and more uniform bonds, a compatible primer or adhesion promoter may be used on surfaces other than rubber and silicone rubber. Store the product in its original unopened container at or below 32°C.

Substrate and use limitations

The sealant is not recommended for continuous underwater immersion where adhesion or structural bonding is required, masonry, painted-over surfaces or totally confined areas. Adhesion is limited on PTFE-coated materials, polyethylene, polypropylene and methyl methacrylate. Acetic acid released during cure may corrode sensitive metals, and some plastics may develop stress cracking; evaluate the complete substrate and cure configuration before use.

After cure

Cured and service properties

Typical cured values were measured after 72 hours at 25°C and 50% relative humidity and are not intended as guaranteed specifications.

Property Typical value Unit or condition
Durometer hardness 26 Shore A points
Tensile strength 350 psi
Elongation 600 %
Continuous operating temperature -65 to 260 °C
Intermittent temperature exposure 315 °C maximum stated exposure
Applications

Product applications

The product’s stated temperature range and nonslumping consistency support bonding and sealing applications around equipment and components exposed to elevated operating temperatures.

Appliance heating element assembly sealed and encapsulated with red high-temperature silicone
Appliance heating elements
Sealing and encapsulating heating elements in appliances where the cured silicone is exposed to sustained elevated temperatures.
Industrial oven and moving oven belt components with high-temperature silicone sealing points
Industrial ovens and moving belts
Bonding and sealing around industrial ovens and moving oven-belt equipment requiring a nonslumping silicone for high-temperature exposure.
Aerospace gasket and smoke-stack bag-filter assemblies using red high-temperature silicone sealant
Aerospace gasketing and bag filters
Applications include aerospace gasketing and sealing bag filters on smoke stacks where parts must operate at high temperatures.
Product resources

Supporting technical resources

Use these supporting documents to review silicone options for powertrain systems, compare adhesive-sealant choices for vehicle system design and examine supplier documentation related to material screening.

Technical guide · PDF
Dow silicone options for vehicle powertrain systems
Reviews silicone material options and application considerations for sealing, gasketing and protecting components within vehicle powertrain systems.
Open the vehicle powertrain systems guide
Selection guide · PDF
Dow adhesive-sealant solutions for vehicle system design
Supports comparison of Dow adhesive and sealant technologies by vehicle-system application, processing characteristics and material-selection requirements.
Open the vehicle system selection guide
Supplier letter · PDF
Red List-free letter — DOWSIL™ 736 Heat Resistant Sealant
Provides supplier documentation addressing Red List screening for DOWSIL™ 736 Heat Resistant Sealant for teams evaluating project-specific material requirements.
Open the supplier material letter
Next steps

Technical support for DOWSIL™ 736

Need help evaluating DOWSIL™ 736 for a high-temperature joint, gasket, heating element or equipment assembly? Krayden can help review substrate compatibility, surface preparation, cure access, section thickness and operating-temperature requirements before application testing.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers