DOWSIL 733

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 733

Main features

  • Non-Slumping Vertical/Overhead Application
  • Primerless Glass, Metal, and Plastic Adhesion
  • -57 to 177 deg C Flexibility

Product Description

DOWSIL™ 733 Glass & Metal Sealant is a one-part, acetoxy-cure silicone rubber supplied as a nonslumping paste for OEM bonding and sealing. It adheres without primer to many properly cleaned glass, metal and plastic substrates and cures at room temperature through exposure to atmospheric moisture. Applications include appliances, heavy equipment, marine equipment and recreational vehicles.

Key features

  • Nonslumping consistency: Supports application on vertical, sidewall and overhead surfaces without sagging or running.
  • Unprimed adhesion: Adheres to many properly cleaned glass, metal and plastic substrates without primer.
  • Broad flexibility range: Remains flexible from -57 to 177°C, with intermittent exposure to 204°C.

Applications

OEM bonding and sealing for appliances, heavy equipment, marine equipment and recreational vehicles.

Technical Specifications

General Properties
Color
The color
Clear, white, black and aluminum
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.03
Physical Properties
Tack-Free Time
15 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %

Additional Information

Industrial silicone sealant

DOWSIL™ 733 Glass & Metal Sealant

A one-part, acetoxy-cure silicone rubber for OEM bonding and sealing. The ready-to-use nonslumping paste adheres without primer to many properly cleaned glass, metal and plastic substrates and cures through exposure to atmospheric moisture to form a tough, flexible rubber.

One-part silicone Acetoxy moisture cure Nonslumping paste Primerless adhesion Flexible after cure
DOWSIL 733 Glass and Metal Sealant in its commercial product packaging

DOWSIL™ 733 Glass & Metal Sealant; packaging and available color may vary.

Uncured material

As-supplied properties

Typical values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Standard colors Clear, white, black and aluminum — Standard commercial colors
Specific gravity 1.03 — At 25°C
Extrusion rate 350 g/min 3.18 mm orifice; 90 psi air pressure
Flow rate — sag or slump Nil mm 3.18 × 101.6 mm bead
Tack-free time 15 minutes 25°C and 50% relative humidity
Cure time 24 hours 3.18 mm thickness at 25°C and 50% relative humidity
Shelf life 900 days Store in the original unopened container at or below 32°C
Processing

Application and cure

DOWSIL™ 733 is supplied ready to use and extrudes directly from its container. Apply it to properly prepared surfaces in a uniform thickness, complete tooling before the tack-free skin forms and allow the assembly to remain undisturbed at room temperature during cure.

Surface preparation: Thoroughly clean and degrease applicable metal and plastic surfaces with a suitable solvent. Roughen rubber surfaces with sandpaper, then wipe with acetone.
Application and tooling: Force the sealant into the joint or seam to obtain full surface contact. Tool within approximately 5 to 10 minutes and remove masking tape before a tack-free skin forms.
Cure conditions: A tack-free skin forms in approximately 10 to 15 minutes at 25°C and 50% relative humidity. Sections up to 3.18 mm thick become rubbery solids in about 24 hours under these conditions.
DOWSIL 733 sealant being dispensed and tooled into a properly prepared industrial joint

Apply a uniform bead to properly prepared surfaces and complete tooling before skin formation.

Storage and handling

Store the product in its original unopened container at or below 32°C. Cure progresses inward from surfaces exposed to atmospheric moisture. Lower humidity, greater section thickness and confinement extend cure time; complete cure may not occur under absolute confinement. Follow the applicable solvent label and current safety documentation when preparing surfaces and handling the product.

Cured silicone rubber

Cured properties

Typical values are not intended for use in preparing specifications. Cure conditions and test context are shown with each property.

Property Typical value Unit or condition
Durometer hardness 25 Shore A; ASTM D2240; cured 3 days at 25°C and 50% RH
Tensile strength 2.3 (335) MPa (psi); ASTM D412, Die C; cured 3 days
Elongation 500 %; ASTM D412, Die C; cured 3 days
180° peel strength — stainless steel 20 pli; cured 2 days at 25°C and 50% RH
180° peel strength — matte-finish steel 20 pli; cured 2 days at 25°C and 50% RH
180° peel strength — aluminum 21 pli; cured 2 days at 25°C and 50% RH
Sustained flexibility range -57 to 177 °C; intermittent exposure to 204°C
Supported use contexts

Applications

DOWSIL™ 733 is used for OEM bonding and sealing in industrial and transportation-related equipment assemblies.

Appliance assembly containing a bonded or sealed glass-to-metal interface
Appliance assemblies
Used for OEM bonding and sealing of appliance components, including properly prepared glass, metal and plastic interfaces.
Heavy equipment enclosure or panel joint prepared for industrial silicone sealing
Heavy equipment
Used in heavy-equipment bonding and sealing applications requiring a nonslumping, flexible silicone rubber.
Marine or recreational vehicle panel and window interface prepared for silicone sealing
Marine and recreational vehicle equipment
Used for OEM bonding and sealing in marine equipment and recreational vehicle assemblies exposed to vibration, moisture and weather.

Product resources

DOWSIL™ Silicone Sealants and Foams for Industrial, Appliance and Maintenance
A selection guide covering Dow silicone-sealant chemistries, product options, typical properties and industrial, appliance and maintenance applications.
View resource
Certified Solutions for Food and Beverage Processing
An application-focused guide to Dow material solutions and certification considerations for equipment used in food-and-beverage processing environments.
View resource
Next steps

Evaluate DOWSIL™ 733 for your bonding or sealing application

Contact Krayden to discuss substrate preparation, joint geometry, cure access, production conditions and service-temperature requirements. Product-specific testing should confirm adhesion, cure and performance with the intended substrates and assembly design.

Leading Brands Trust in Our Products and Services