DOWSIL 7092

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 7092

Main features

  • Immediate Green Strength
  • One-Component, Neutral Moisture-Cure Formulation
  • Flexible Cured Adhesive

Product Description

DOWSIL™ 7092 High Green Strength Adhesive and Sealant is a one-component, neutral-cure silicone adhesive and sealant that develops immediate green strength after application. Its fast initial strength supports earlier handling and processing of bonded units while moisture cure continues at room temperature. The non-sag, paste-like material cures to a tough, flexible rubber and remains stable and flexible from -50°C to 150°C. It provides unprimed adhesion to commonly used materials including certain steels, aluminum, glass, polycarbonate, PA, and PBT, while plasma treatment may support adhesion to selected PP, PMMA, and ABS substrates. Preliminary application testing remains necessary, particularly for low-energy plastics.

Key features

  • Immediate green strength: Builds handling strength directly after application to support faster movement of bonded assemblies through production.
  • One-component neutral moisture cure: Cures at room temperature without component mixing and forms a tough, flexible silicone rubber.
  • Non-sag application and broad evaluated adhesion: Paste consistency supports controlled bead application on assemblies using selected glass, metal, and engineering-plastic substrates.

Applications / Suitable for

  • Bonding and sealing applications requiring immediate handling or continued processing
  • Assemblies using glass with selected steel or aluminum substrates
  • Assemblies using selected engineering plastics, subject to substrate-specific adhesion testing

Technical Specifications

General Properties
Color
The color
Black, white
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.55
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
435 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and application-stage properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Available colors Black, white — As supplied
Appearance Paste-like — As supplied; non-sag consistency
Extrusion rate 217 g/min CTM 0364 / ASTM D2452; 3.18 mm nozzle at 0.62 MPa
Skin-over time 15–25 min CTM 0095; tack-free surface at room temperature and 50% relative humidity

After-processing / final-state properties

Typical cured-material and lap-shear properties after seven days at 23°C and 50% relative humidity. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Durometer hardness 55 Shore A CTM 0099 / ASTM D2240
Modulus at 100% elongation 1.2 MPa CTM 0137A / ASTM D412
Tensile strength 2.0 MPa CTM 0137A / ASTM D412
Elongation at break 435 % CTM 0137A / ASTM D412
Specific gravity 1.55 — CTM 0097F; measured at 23°C
Lap-shear strength on metals 1.1–1.4 MPa Approximate range for tested steel and aluminum lap-shear assemblies
Lap-shear strength on plastics 1.3–1.4 MPa Tested PC, PA, and PBT lap-shear assemblies
Lap-shear strength on plasma-treated plastics 1.2–1.4 MPa Tested plasma-treated PP, PMMA, and ABS lap-shear assemblies