DOWSIL 520

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL 520

Main features

  • Water-Dilutable 40% Active Emulsion
  • Deep Mineral-Substrate Penetration
  • Substrate-Specific Water Repellency

Product Description

DOWSIL 520 Dilutable Water Repellent Emulsion supplies a milky-white, water-dilutable silane/siloxane emulsion containing 40% active material for formulating penetrating water-repellent treatments. It can be used as supplied or diluted with water for mineral substrates such as brick, stone, concrete and mortar. After application, the active molecules penetrate absorbent surfaces and react to form a hydrophobic treatment that inhibits water absorption while retaining the substrate's original appearance. Laboratory water-exclusion results vary with substrate and active-solids concentration, so dilution should be selected using test applications on the specific surface.

Key features

  • 40% active emulsion: Can be used as supplied or diluted with water for treatment formulation.
  • Penetrating mineral treatment: Small active molecules support penetration into absorbent masonry surfaces.
  • Condition-specific water exclusion: Performance is separated by substrate and active-solids level.

Applications

Penetrating water-repellent treatments for brick, stone, concrete and mortar.

Technical Specifications

General Properties
Color
The color
Milky White
Density (g)
0.97 g/cm3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.965
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
> 100 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied emulsion properties. Values are not specifications.

Property Value Unit Method / condition
Color Milky white As supplied
Nonvolatile content 40 % Typical active content
pH 4.5 Typical value
Specific gravity 0.985 At 25 deg C
Flash point >100 deg C Closed cup
Density 8.216 lb/gal Typical value
VOC content <300 g/L Typical value
Solvent / thinner Water As supplied
Technical properties

After-processing / final-state properties

Laboratory water-repellency results for treated mineral substrates. Performance varies with substrate and active-solids concentration.

Property Value Unit Method / condition
Water exclusion, mortar cubes 92 / 94.8 / 93.9 % After 24 hr immersion; 5% / 10% / 20% active solids; ASTM C642
Water exclusion, cement brick 63.9 / 77 / 82.5 % After 24 hr immersion; 5% / 10% / 20% active solids; modified ASTM C67
Water exclusion, Belden brick 80.3 / 69.8 / 41.1 % After 24 hr immersion; 5% / 10% / 20% active solids; modified ASTM C67
Water exclusion, Glen Gary brick 77.7 / 48.3 / 43.3 % After 24 hr immersion; 5% / 10% / 20% active solids; modified ASTM C67
Water exclusion, mortar cubes 74.0 % After 21 days immersion; 40% active solids; modified NCHRP 244
Penetration, mortar cubes 4-5 mm 40% active solids; modified NCHRP 244
Leak-rate reduction, concrete block 76 % 5% active solids; modified ASTM E514
Penetration, concrete block 15 mm 5% active solids; modified ASTM E514

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers