DOWSIL™ 510 Fluid is a phenylmethyl polysiloxane silicone fluid for hydraulic, motion-dampening, and heat-transfer applications. Available in nominal viscosities from 50 to 30,000 cSt, it combines high-temperature stability during continuous use at 232°C (450°F) with an estimated pour point as low as -57°C (-70°F), depending on viscosity. Its high flash point, low volatility, oxidation resistance, and relatively constant thermal conductivity support evaluation in demanding fluid systems, including hydraulic arrestors, hydraulically actuated valves and instruments, and heat-transfer equipment.

Key features

  • Broad viscosity selection: Available in 50, 100, 500, and 30,000 cSt grades for different hydraulic and damping requirements.
  • Wide temperature capability: Demonstrates high-temperature stability during continuous use at 232°C (450°F), with an estimated pour point as low as -57°C (-70°F).
  • High-temperature fluid properties: Provides a minimum flash point of 274°C (525°F), an estimated fire point above 343°C (650°F), and low volatility.

Applications

  • Hydraulic arrestors and motion-dampening systems
  • Hydraulically actuated valves and instruments used in nuclear plants
  • High- and low-temperature heat-transfer systems

Technical Specifications

General Properties
Color
The color
40
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.11
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
302 °C

Additional Information

Hydraulic and heat-transfer fluid

DOWSIL™ 510 Fluid

A phenylmethyl polysiloxane silicone fluid available in multiple viscosities for hydraulic arrestors, motion-dampening systems, hydraulically actuated equipment, and heat-transfer applications. It combines wide-temperature capability with high flash and fire points, low volatility, and chemical inertness.

50–30,000 cSt range 232°C continuous use 274°C minimum flash point Low volatility Phenyl silicone chemistry
DOWSIL™ 510 Fluid product container for hydraulic and heat-transfer fluid applications

DOWSIL™ 510 Fluid is supplied in multiple nominal viscosities and container sizes.

As supplied

Available grades and physical properties

Values shown are typical and are not intended for use in preparing specifications.

Property Value Unit Condition or context
Viscosity 50, 100, 500, 30,000 cSt At 25°C (77°F)
Specific gravity 0.985, 0.992, 0.997, 0.990 — At 25°C (77°F); values correspond respectively to the listed viscosity grades
Color 20, 20, 20, 50 APHA Values correspond respectively to the listed viscosity grades
Packaging 8, 40, 440 lb Equivalent net weights: 3.6, 18.1, and 200 kg
System integration

Fluid selection and compatibility

Select the viscosity grade according to the hydraulic, damping, or heat-transfer system requirements. Evaluate fluid compatibility and elastomer interactions before introducing DOWSIL™ 510 Fluid into an existing system.

Viscosity selection: Available nominal viscosity grades are 50, 100, 500, and 30,000 cSt at 25°C (77°F).
Silicone-fluid compatibility: DOWSIL™ 510 Fluid is incompatible with DOWSIL™ 550 Fluid and DOWSIL™ 710 Fluid. Determine compatibility before use with other silicone fluids.
Elastomer interaction: The fluid can swell silicone rubber. Confirm the suitability of seals and other elastomeric materials under the intended operating conditions.
Illustration of a closed hydraulic or heat-transfer system showing fluid circulation, seals, valves, and compatibility evaluation points

Representative hydraulic or heat-transfer system

Storage and handling

Store DOWSIL™ 510 Fluid in its original, unopened container at 25°C (77°F). It has no known limit to useful life under these conditions; Dow warrants product shelf life for up to 60 months from the date of manufacture. Review the current product and safety information before handling.

In-use performance

Thermal and fluid properties

Values shown are typical unless identified as minimum or estimated and are not intended for use in preparing specifications.

Property Typical value Unit or condition
Viscosity/temperature coefficient 0.655 —
Flash point, minimum 274 (525) °C (°F)
Fire point, estimated >343 (>650) °C (°F)
Autoignition temperature, estimated 482 (900) °C (°F)
Pour point, estimated -57 (-70) °C (°F)
Specific heat 0.405 At 100°C (212°F)
Thermal conductivity 0.00036 g-cal/cm²-sec-°C at 50°C (122°F)
Volatile content 2.5 % by weight after 4 hours at 250°C (482°F)
Compression 2.80 / 7.95 % at 5,000 / 20,000 psi; 100 cSt grade
Bulk modulus 179,000 / 253,000 At 5,000 / 20,000 psi; 100 cSt grade

Pour-point results may be affected by cooling rate and may be lower than the temperature at which the fluid melts. Evaluate multiple lots when low-temperature phase behavior is critical to the application.

Applications

Hydraulic, damping, and heat-transfer uses

DOWSIL™ 510 Fluid is used where hydraulic response, compressibility, temperature resistance, and heat-transfer capability are important evaluation factors.

Hydraulic arrestors and snubbers
The fluid’s relatively high compressibility supports use in hydraulic arrestors and other systems requiring shock absorption or motion damping.
Hydraulically actuated valves and instruments
Applications include hydraulically actuated valves, subject to system-specific engineering and qualification requirements.
Heat-transfer systems
Its oxidation resistance, temperature resistance, and relatively constant thermal conductivity support evaluation as a heat-transfer fluid across a wide temperature range.

Product resources

Dow fluid resistance product guide
Review supporting compatibility and fluid-resistance information when evaluating materials used with DOWSIL™ silicone fluids in hydraulic or heat-transfer systems.
View resource
Typical properties of DOWSIL™ silicone fluids
Explore broader property information for DOWSIL™ silicone fluids to support fluid selection, engineering comparison, and application evaluation.
View resource
Next steps

Evaluate DOWSIL™ 510 Fluid for your system

Krayden can help review viscosity selection, operating-temperature requirements, fluid compatibility, packaging options, and application-specific considerations for hydraulic, motion-dampening, or heat-transfer systems using DOWSIL™ 510 Fluid.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers