DOWSIL™ 3-6876 Adhesive is a one-part, flowable, addition-cure silicone adhesive for bonding, sealing, and gasketing applications in electronic and automotive assemblies. The black adhesive requires no mixing and can be applied by automated or manual needle dispensing. Its 41,275 mPa·s typical viscosity allows the material to flow, fill, and self-level after dispensing. Cure speed is controlled by temperature, with typical schedules ranging from 300 minutes at 100°C to 30 minutes at 150°C. After cure, the material provides 5.5 MPa tensile strength, 255% elongation, Shore A 53 hardness, and 4.4 MPa unprimed lap-shear adhesion to aluminum. Applications include sealing housings and connectors, attaching baseplates, gasketing, engine and transmission controllers, ABS assemblies, and lighting components.

Key features

  • One-part addition-cure silicone: Requires no component mixing and generates no cure by-products.
  • Flowable, self-leveling consistency: Typical viscosity of 41,275 mPa·s supports needle dispensing, filling, and leveling after application.
  • Temperature-controlled heat cure: Typical cure schedules include 300 minutes at 100°C, 60 minutes at 125°C, and 30 minutes at 150°C.
  • Mechanical strength with elongation: Typical cured properties include 5.5 MPa tensile strength and 255% elongation.
  • Unprimed adhesion to aluminum: Typical lap-shear strength is 4.4 MPa on the tested aluminum configuration.
  • No added solvents: Supplied as a solventless, black silicone adhesive.

Applications / Suitable for

  • Sealing lids, housings, and connectors
  • Attaching baseplates
  • Formed-in-place gasketing
  • Engine, transmission, and ABS controllers
  • Lighting assemblies

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.31
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
255 %

Additional Information

Silicone adhesives

DOWSIL™ 3-6876 Adhesive

A one-part, black, flowable silicone adhesive that combines temperature-controlled heat curing with high tensile strength and elongation. It requires no mixing and can be dispensed manually or with automated needle equipment for bonding, sealing, filling, and gasketing operations.

One-part system Addition heat cure 41,275 mPa·s viscosity Flowable and self-leveling No added solvents
Container of DOWSIL 3-6876 black silicone adhesive

DOWSIL™ 3-6876 Adhesive is supplied as a one-part black silicone adhesive.

Uncured material

As-supplied properties

Viscosity
41,275 mPa·s
Typical uncured viscosity supporting flow, filling, and needle dispensing.
Component count
One part
All ingredients required for addition curing are supplied in the material; no mixing is required.
Appearance
Black liquid
Flowable silicone elastomer supplied without added solvent.
Application method
Needle dispense
Suitable for automated or manual needle-dispensing equipment.
Application and processing

Processing and cure

Thoroughly mix the material before use when filler settling has occurred. Prepare clean, degreased substrates, dispense the adhesive, assemble the parts, and apply a supported heat-cure schedule. Cure rate increases with temperature.

Dispensing
Automated or manual needle dispense
Cure at 100°C
300 minutes typical
Cure at 125°C
60 minutes typical
Cure at 150°C
30 minutes typical

 

Storage and handling

Store the material in its original, tightly closed container. The reported shelf life is 12 months at 5°C. Cold storage is recommended to extend usable life, and the product label “Use Before” date should be observed. Protect the material from moisture and incompatible cure-inhibiting substances.

Typical heat-cure schedules
Cure temperature Typical cure time Processing context
100°C 300 minutes Lower-temperature schedule with the longest listed cure time.
125°C 60 minutes Intermediate cure schedule.
150°C 30 minutes Highest-temperature and shortest listed cure schedule.

For thick sections or when voiding is observed, a 30-minute pre-cure at 70°C may be evaluated. Cure schedules and adhesion should be confirmed in the actual assembly.

Final material state

Cured properties

Tensile strength
5.5 MPa
Typical cured tensile strength.
Elongation
255%
Typical tensile elongation of the cured silicone.
Aluminum lap shear
4.4 MPa
Typical unprimed lap-shear adhesion on the tested aluminum configuration.
Hardness
Shore A 53
Typical cured elastomer hardness.
Typical cured-property data
Property Typical value Context
Specific gravity 1.311 Cured material
Tensile strength 5.5 MPa / 795 psi Typical cured tensile result
Elongation 255% Typical tensile elongation
Tensile modulus 2.2 MPa / 310 psi Typical cured tensile modulus
Hardness Shore A 53 Cured elastomer
Unprimed lap shear to aluminum 4.4 MPa / 640 psi Specific to the tested aluminum and joint configuration
Linear coefficient of thermal expansion 250 ppm/°C Measured by thermomechanical analysis
General long-term operating range −45 to 200°C Application performance must be verified in the actual part and operating conditions

Values are typical and are not intended as product specifications or design allowables.

Documented use contexts

Applications

The flowable one-part material can be evaluated for dispensing into bonded and sealed assemblies that can accommodate the required heat-cure process.

Electronic or automotive housing with a dispensed silicone adhesive bead for lid sealing

Housing, lid, and connector sealing

Flow and self-leveling after dispensing support the formation of adhesive and sealing beads around lids, housings, and connector interfaces.

Baseplate being bonded to an electronic control module housing with dispensed silicone adhesive

Baseplate attachment and gasketing

The product can be used for attaching baseplates and forming gaskets in assemblies where one-part dispensing and heat curing are compatible with the production process.

Automotive electronic control modules and lighting assemblies using bonded or sealed housings

Controllers and lighting assemblies

Applications include engine, transmission, and ABS controllers as well as lighting components requiring bonded or sealed housings.

Supporting literature

Product resources

Review broader silicone adhesive-selection and electronics-application guidance to place DOWSIL™ 3-6876 Adhesive within relevant material and manufacturing contexts.

Selection guide

Advanced Silicone Adhesives and Sealants Guide

Provides broader guidance on silicone adhesive and sealant technologies, processing approaches, performance characteristics, and product-selection considerations.

Open the silicone adhesives and sealants guide
Application guide

Material Solutions for Communications and Consumer Applications

Reviews silicone-material roles in communications and consumer electronics, including bonding, sealing, protection, assembly, and thermal-management applications.

Open the communications and consumer applications guide

Technical support for DOWSIL™ 3-6876 Adhesive

Need help matching DOWSIL™ 3-6876 Adhesive to a housing, baseplate, connector, gasket, or controller assembly? Krayden can support material selection, dispensing evaluation, substrate and adhesion testing, and development of a suitable heat-cure process.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers