DOWSIL 3-4680

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 3-4680

Main features

  • Fast Room-Temperature Encapsulation Cure
  • Low-Viscosity Dispensing Control
  • Electrically Insulating Encapsulation

Product Description

DOWSIL™ 3-4680 Silicone Gel Kit is a two-part, addition-cure silicone dielectric gel supplied in a 1:1 mix ratio. The transparent blue, low-viscosity material cures rapidly at room temperature to form a soft gel for sealing, encapsulating, and potting electronic devices. Its short working time and room-temperature cure support applications requiring rapid processing, while heat can be used to further accelerate cure. After processing, the gel combines high volume resistivity and dielectric strength with the soft, resilient characteristics associated with silicone gel protection.

Key features

  • Fast room-temperature cure: Reaches 90% of final properties in approximately 15 minutes at room temperature.
  • Low-viscosity processing: Typical viscosity of 275 mPa·s supports dispensing and filling before gelation.
  • Dielectric performance: Typical dielectric strength of 400 V/mil (16 kV/mm) and volume resistivity of 3.60 × 1015 ohm-cm after cure.

Applications / Suitable for

  • Sealing electronic devices
  • Electronic encapsulation and potting
  • Protection of delicate electronic components
  • Applications requiring cushioning against mechanical shock and vibration
Product Family

DOWSIL 3-4680

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
275 mPa.s
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.97
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
16 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
3.60E15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties for the two-part silicone gel before and during initial processing.

Property Value Unit Method / condition
Cure system Addition cure — Two-part system; 1:1 mix ratio
Color Transparent blue — Typical
Viscosity 275 mPa·s Typical; equivalent to centipoise
Specific gravity 0.97 — Cured or uncured Parts A and B
Working time <10 min Time for initial mixed viscosity to double at room temperature
Shelf life 12 months From date of manufacture in the original unopened container, stored below 35°C

After-processing / final-state properties

Typical properties measured after the mixed silicone has cured to form a soft dielectric gel.

Property Value Unit Method / condition
Penetration 60 1/10 mm Typical cured-gel value
Gel hardness 90 g Typical cured-gel value
Dielectric strength 400 / 16 V/mil / kV/mm Typical cured-gel value
Dielectric constant 2.75 / 2.75 — At 100 Hz / 100 kHz
Volume resistivity 3.60 × 1015 ohm-cm Typical cured-gel value
Dissipation factor 0.0004 / <0.00006 — At 100 Hz / 100 kHz
Linear coefficient of thermal expansion 435 µm/(m·°C) Typical cured-gel value