DOWSIL 3-0115 Automotive Sealant

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 3-0115 Automotive Sealant

Main features

  • Automotive Powertrain-Fluid Resistance
  • Blowout-Resistant In-Line Leak Testing
  • Primerless Metal and Plastic Adhesion

Product Description

DOWSIL™ 3-0115 Automotive Sealant is a one-part, self-priming, noncorrosive alkoxy-cure RTV silicone rubber developed for automotive powertrain sealing. Supplied as a high-viscosity, nonslumping paste, it forms an elastomeric seal resistant to most automotive powertrain fluids and is formulated to withstand in-line pressure leak testing during assembly. The sealant exhibits excellent unprimed adhesion to properly prepared metals and many plastics, while its low oil-foaming behavior supports use with automatic transmission fluids and engine oils. These characteristics make it suitable for automotive flange sealing across engine, transmission, axle, and coolant-system assemblies, subject to application-specific process validation and qualification.

Key features

  • One-part alkoxy-cure RTV system - Self-priming, noncorrosive silicone rubber that cures through exposure to atmospheric moisture.
  • Powertrain fluid resistance - Forms an elastomeric seal resistant to most automotive powertrain fluids.
  • Blowout resistance - Formulated to withstand in-line pressure leak testing during assembly operations.
  • Unprimed adhesion - Exhibits excellent adhesion to properly prepared metals and many plastics.
  • Low oil foaming - Provides low-foaming behavior in contact with automatic transmission fluids and engine oils.
  • Nonslumping paste consistency - High-viscosity paste suitable for manual application or automated dispensing.
  • Low-odor formulation - Supports automotive sealing operations where material odor is a processing consideration.

Applications / Suitable for

  • Automotive flange sealing
  • Assemblies requiring immediate pressure leak testing
  • Engine and transmission oil pan sealing
  • Differential and axle cover sealing
  • Coolant-system sealing
  • Engine block main seals

Technical Specifications

General Properties
Color
The color
Gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.29
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
375 %

Additional Information

Automotive adhesive and sealant

DOWSIL 3-0115 Automotive Sealant

DOWSIL 3-0115 Automotive Sealant is a one-part, self-priming, noncorrosive alkoxy-cure RTV silicone rubber for automotive powertrain sealing. Its high-viscosity, nonslumping paste is formulated for fluid-resistant elastomeric sealing and in-line pressure leak testing, with excellent unprimed adhesion to properly prepared metals and many plastics and low oil-foaming behavior in transmission fluids and engine oils.

One-part RTV siliconeAlkoxy moisture cureHigh-viscosity nonslumping pasteNoncorrosiveLow oil foaming
Technical properties

Typical as-supplied properties

Values are typical and are not intended for use in preparing specifications. Unless otherwise indicated, conditions are 23 deg C (73 deg F) and 50% relative humidity. CTMs are Corporate Test Methods and correspond to standard ASTM tests in most instances.

Property Value Unit Method / condition
Consistency High-viscosity, nonslumping paste - CTM 0176; 23 deg C (73 deg F), 50% relative humidity
Color Gray - CTM 0063; 23 deg C (73 deg F), 50% relative humidity
Extrusion rate 50 g/minute CTM 0364; 3.2-mm (1/8-inch) nozzle at 0.63 MPa (90 psi)
Skin-over time 10 minutes CTM 0098; 23 deg C (73 deg F), 50% relative humidity
Tack-free time 20-25 minutes CTM 0095; 23 deg C (73 deg F), 50% relative humidity
Cure rate, 3.2 mm (1/8 inch) 24 hours CTM 0084; 23 deg C (73 deg F), 50% relative humidity
Specific gravity 1.29 - CTM 0097; 23 deg C (73 deg F), 50% relative humidity
Volatility 0.3 % CTM 0087; 23 deg C (73 deg F), 50% relative humidity
Processing

Application and cure

DOWSIL 3-0115 is a one-part moisture-cure RTV sealant. Surface condition, bead geometry, ambient humidity, exposed area, and assembly timing affect application and cure behavior.

Surface preparation: Surfaces to be sealed or adhered should be free of dirt, oil, and other contaminants. A surface primer may be recommended for hard-to-bond surfaces such as some plastics.
Application: Apply in a continuous, uniform thickness. Bead size depends on the anticipated part gap and flange width.
Dispensing: Manual application is possible; automated dispensing is highly recommended where a uniform seal is required.
Assembly timing: At room temperature and 50% relative humidity, the surface skins over in about 10 minutes. Assemble mating parts before skin-over.
Moisture cure: A fully exposed section cures inward to a depth of 3.2 mm in 24 hours at room temperature and 50% relative humidity. Lower humidity or confined joints extend cure time.
Storage: Store at or below 32 deg C (90 deg F) in original, unopened containers.
Cured material

Typical cured properties

Values apply after curing for 7 days at 23 deg C (73 deg F) and 50% relative humidity. These are typical test results, not guaranteed design values.

Property Value Unit Method / condition
Durometer, Shore A 50 - ASTM D2240; after 7 days cure at 23 deg C (73 deg F), 50% relative humidity
Tensile strength 2.80 (405) MPa (psi) ASTM D412; after 7 days cure at 23 deg C (73 deg F), 50% relative humidity
Elongation 375 % ASTM D412; after 7 days cure at 23 deg C (73 deg F), 50% relative humidity
Lap shear adhesion, 2024 aluminum 2.4 (350) MPa (psi) ASTM D816; 12.7 x 25.4 x 1 mm (0.5 x 1 x 0.040 inch); after 7 days cure at 23 deg C, 50% relative humidity
Lap shear adhesion, 1010 steel 2.3 (330) MPa (psi) ASTM D816; 12.7 x 25.4 x 1 mm (0.5 x 1 x 0.040 inch); after 7 days cure at 23 deg C, 50% relative humidity
Applications

Automotive sealing applications

DOWSIL 3-0115 is positioned for automotive powertrain sealing, with exact-product application support across flange, oil, axle, coolant, and related sealing contexts.

Flange and static engine sealing
Applications include automotive flange sealing and engine block main seals. Dow selection guidance also lists DOWSIL 3-0115 as a one-part adhesive seal option for static engine seals with on-line pressure checking.
Engine, transmission and axle sealing
Applications include engine and transmission oil pans and axle cover seals. Dow vehicle-system guides also list the product among adhesive-seal options for transmission or gearbox and differential or axle-cover sealing.
Coolant and auxiliary powertrain sealing
Applications include coolant system seals. Dow vehicle-system guides also identify DOWSIL 3-0115 among adhesive-seal options for thermostat housing and fan-clutch sealing contexts.
Product resources

Application and selection resources

Use these supporting resources to review exact-product information, documented application contexts, and Dow vehicle-system selection guidance.

Web resource
Official Dow product page
Current exact-product overview with uses, benefits, cure classification, and selected typical properties for DOWSIL 3-0115 Automotive Sealant.
View official product page
Case study
Dow Solution Enables Manufacturer to Meet New Axle Sealing Test Standards
Documents a customer-specific axle-sealing evaluation program covering adhesion, oil immersion, high-temperature and oil-foaming testing, followed by field evaluation and dispensing integration.
View axle sealing case study
Selection guide
Silicone Options for Vehicle Powertrain Systems
Places DOWSIL 3-0115 within Dow's powertrain selection framework for fan-clutch, thermostat-housing, transmission, differential or axle-cover, and static-engine sealing.
View powertrain selection guide
Selection guide
Adhesive and Sealant Solutions for Vehicle System Design
Provides broader vehicle-system selection context and identifies DOWSIL 3-0115 among adhesive-seal options for multiple documented automotive applications.
View vehicle system selection guide
Next steps

Evaluate DOWSIL 3-0115 for your sealing process

Krayden can help review flange geometry, substrate preparation, bead and dispensing considerations, assembly timing, cure conditions, and the fluid or leak-test requirements relevant to evaluating DOWSIL 3-0115 Automotive Sealant. Contact us to discuss application fit, technical data, sampling, or qualification planning for your automotive sealing process.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers