DOWSIL 20

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 20

Main features

  • Heat-Stable Non-Carbonizing Parting Film
  • Solvent-Dilutable Release Formulation
  • Plastic/Adhesive/Elastomer Product Applications

Product Description

DOWSIL™ 20 Release Coating is a solvent-based silicone release coating formulated for plastics, adhesives, and elastomeric products. The colorless to light-straw liquid contains polydimethylsiloxane and high-molecular-weight silicone resin and forms a durable, non-oily parting film on prepared mold surfaces. It can be diluted with suitable aliphatic or aromatic hydrocarbon solvents and applied by spraying, brushing, or wiping. In most cases, one application supports release through multiple molding cycles while minimizing buildup on molds and dies. An optional heat treatment of 5 to 10 minutes at 93 to 204°C can improve release and film durability.

Key features

  • Durable release film: Forms a heat-stable, non-carbonizing, non-oily parting layer that can provide release through numerous molding cycles.
  • Solvent-dilutable application: May be diluted for application control and applied to cleaned mold surfaces by spraying, brushing, or wiping.
  • Low mold buildup: Supports release with minimal accumulation on molds and dies and does not discolor molded parts.

Applications / Suitable for

  • Molding epoxies, melamines, methacrylates, phenolics, polyesters, and polyurethanes
  • Releasing silicone-glass laminates, tubes, and parts made from silicone molding compounds
  • Wood-forming operations, metalworking, and rubber-gasket production
Product Family

DOWSIL 20

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
colorless
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.93
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Composition Polydimethylsiloxane and high-molecular-weight silicone resin in solvent — As supplied; solvent-based release coating
Color Colorless to light straw — CTM 0005
Active material content 50 % w/w CTM 0208
Specific gravity 0.93 g/mL CTM 0001A; at 25°C (77°F)
Kinematic viscosity 11.0 cSt CTM 0004
Flash point, closed cup 32 °C CTM 0021A
Solvent Stoddard solvent and xylene — Suitable dilution solvents include aliphatic and aromatic hydrocarbons

Leading Brands Trust in Our Products and Services