DOWSIL 1201

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 1201

Main features

  • Adhesion-Promoting Surface Treatment
  • Low-Viscosity Adhesive Application
  • 1 to 2-Hour Cure Window

Product Description

DOWSIL™ 1201 RTV Prime Coat is a one-part, light yellow silicone primer formulated to enhance the adhesion of SILASTIC™ RTV-3110, RTV-3112, and RTV-3120 Mold-Making Bases to selected substrates. The acetone/toluene-based liquid deposits a thin layer of silane coupling agents and other active ingredients onto prepared surfaces. It can be applied by wiping, dipping, or spraying and typically cures through exposure to atmospheric moisture for 1 to 2 hours at room temperature and 20 to 90% relative humidity. Supported substrates include metals, glass, wood, masonry, and structural plastics.

Key features

  • Adhesion-enhancing primer: Formulated to improve the bonding of specified SILASTIC™ RTV mold-making elastomers to supported substrate types.
  • Multiple application methods: May be applied in a light, even coat by wiping, dipping, or spraying.
  • Room-temperature moisture cure: Typically cures for 1 to 2 hours at room temperature and 20 to 90% relative humidity before silicone application.

Applications / Suitable for

  • Priming metals and glass before applying supported SILASTIC™ RTV elastomers
  • Priming wood and masonry bonding surfaces
  • Priming supported structural plastics

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-20 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties from the technical data sheet. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Product form One-part liquid primer — Silane coupling agents and other active ingredients diluted in an acetone/toluene solvent mixture
Color Light yellow — As supplied
Non-volatile content 23.32 % CTM 0010; 1 hour at 110°C
Kinematic viscosity 1.11 cSt CTM 0004; at 25°C
Flash point, closed cup −20 °C Equivalent to −4°F
Typical primer cure 1–2 hours Room temperature; 20–90% relative humidity; lower temperature or humidity requires longer cure
Shelf life 12 months At 25°C; store below 32°C and protect from moisture