DOWSIL 1200

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL 1200

Main features

  • No-Mix Primer Application
  • RTV and Heat-Cure Silicone Adhesion
  • Glass, Ceramic, FR-4, and Metal Adhesion

Product Description

DOWSIL™ 1200 OS Primer is a one-part, air-drying adhesion primer supplied as a dilute solution of moisture-reactive materials in volatile siloxane. Applied before silicone bonding or sealing, it improves the quality and speed of adhesion development between room-temperature-vulcanizing silicone materials and a variety of common non-porous substrates. The primer is also suitable for use with heat-curing silicones and can be considered for ceramics, glass, wood, masonry, structural plastics including FR-4, and many metals. Substrate preparation, primer application, and compatibility should be verified for the intended silicone and surface combination.

Key features

  • Air-drying, one-part formulation: Supplied ready for controlled application without component mixing.
  • Silicone adhesion promotion: Supports faster and higher-quality adhesion development for moisture-curing RTV and heat-curing silicones.
  • Broad documented substrate range: Applicable to ceramics, glass, wood, masonry, structural plastics including FR-4, and many metals.

Applications / Suitable for

  • Priming common non-porous substrates before RTV silicone application
  • Adhesion promotion for heat-curing silicone systems
  • Silicone bonding and sealing on glass, ceramics, metals, masonry, wood, and supported structural plastics

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ 1200 OS Primer in its supplied liquid state.

Property Value Unit Method / condition
Number of parts One — As supplied
Appearance Colorless liquid — Heptane-dispersed primer
Flash point 27 °C Closed cup; typical
Volatile organic content 76 g/L Typical
Shelf life 540 days Published product property

Leading Brands Trust in Our Products and Services