DEVCON SF5MIN

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DEVCON SF5MIN

Main features

  • Fast Five-Minute Metal Repair
  • Non-Sag Vertical Rebuilding
  • Machinable Steel-Filled Repairs

Product Description

Devcon Plastic Steel 5-Minute Putty (SF) is a two-component, steel-filled epoxy putty for filling, rebuilding, and bonding metal surfaces. Its putty consistency can be troweled up to 1/4 in (6.4 mm) thick on vertical surfaces without sagging, while a 5-minute pot life at 75 deg F supports rapid repair work. The material reaches functional cure in 1 hour and full cure in 16 hours at room temperature, after which it can be machined, drilled, or painted. Applications include restoring worn metal, patching castings, making jigs and fixtures, and rebuilding pump or valve bodies.

Key features

  • Five-minute working window: The mixed putty has a 5-minute pot life at 75 deg F for rapid repair work.
  • Non-sag vertical repairs: The material can be troweled up to 1/4 in (6.4 mm) thick on vertical surfaces.
  • Machinable steel-filled finish: After full cure, the repair can be machined, drilled, or painted.

Applications / Suitable for

  • Restoring worn or fatigued metal
  • Patching castings and rebuilding pump or valve bodies
  • Making jigs, fixtures, and bearing-journal repairs

Technical Specifications

General Properties
Color
The color
Dark Grey
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.2
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
1.2 kV/mm
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
93 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and mixed properties at 72-75 deg F (23-24 deg C) unless noted.

Property Value Unit Method / condition
Color Dark gray Uncured material
Mix ratio by volume 1:1 Resin to hardener
Mix ratio by weight 1.7:1 Resin to hardener
Mixed viscosity Putty At 72 deg F (23 deg C)
Pot life 5 min At 75 deg F
Specific gravity 2.2 At 72 deg F (23 deg C)
Specific volume 12.2 (0.44) in3/lb (cm^3/g) At 72 deg F (23 deg C)
Technical properties

After-processing / final-state properties

Typical cured properties after 7 days at 75 deg F (24 deg C); values are not specifications.

Property Value Unit Method / condition
Adhesive tensile shear 2,026 (14.0) psi (MPa) ASTM D1002; cured 7 days at 75 deg F (24 deg C)
Compressive strength 10,400 (71.7) psi (MPa) ASTM D695; cured 7 days at 75 deg F (24 deg C)
Flexural strength 7,680 (52.9) psi (MPa) ASTM D790; cured 7 days at 75 deg F (24 deg C)
Hardness 85 Shore D ASTM D2240; cured 7 days at 75 deg F (24 deg C)
Cured shrinkage 0.0006 in/in ASTM D2566; cured 7 days at 75 deg F (24 deg C)
Coefficient of thermal expansion 34 (61.2) x 10^-6 in/in deg F (cm/cm deg C) ASTM D696; cured 7 days at 75 deg F (24 deg C)
Dielectric strength 30 (1.2) V/mil (kV/mm) ASTM D149; cured 7 days at 75 deg F (24 deg C)
Dry temperature resistance 200 (93) deg F (deg C) Cured material