DEVCON PLASTIC WELDER

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DEVCON PLASTIC WELDER

Main features

  • Steel-to-Wood Methacrylate Bonding
  • 3-Minute Open Time
  • 20.6 MPa Cured Tensile Strength

Product Description

DEVCON® Plastic Welder™ White is a two-component, toughened structural adhesive formulated to produce high-strength load-bearing bonds on engineered plastics and other substrates. The room-temperature curing adhesive features a non-sag formulation, a convenient 1:1 mix ratio, and rapid fixture in thin bond lines. It is designed for bonding PVC, fiberglass, ABS, FRT, PPO, PC/PBT, Metton®, Lomod®, Valox®, Noryl®, GTX, Minlon®, epoxy, RIM urethane, wood, and other difficult substrates where outdoor weathering or solvent exposure is anticipated.

Key Features

  • Toughened structural adhesive for high-strength load-bearing bonds on engineered plastics.
  • Room-temperature curing 1:1 system with rapid fixture and non-sag application.
  • Minimal surface preparation required for many bonding applications.

Applications / Suitable for

  • Bonding PVC, ABS, fiberglass and engineered plastics.
  • Bonding epoxy, RIM urethane and wood.
  • Applications exposed to outdoor weathering or solvent exposure.
  • Structural bonding requiring rapid handling strength.
Product Family

DEVCON PLASTIC WELDER

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part A)
45,000 mPa.s
Viscosity (Part B)
40,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
10.5 °C
Operating Temperature
-20 to 120 °C
Mechanical Properties
Peel Strength
6

Additional Information

Adhesives | Toughened Methacrylate Structural Adhesive

Devcon® Plastic Welder

Devcon Plastic Welder is a two-part, room-temperature-curing methacrylate adhesive for load-bearing bonds across supported plastics and dissimilar materials. The 1:1 system forms a non-sagging gel, fixtures rapidly, and provides documented strength on ABS, polycarbonate alloy, grit-blasted steel, and other listed substrates.

1:1 mix ratio 3 min open time 12 min fixture time 20.6 MPa steel lap shear -20 to 120°C service
Devcon Plastic Welder off-white two-part structural adhesive package

Devcon Plastic Welder two-part methacrylate adhesive for supported plastic and mixed-material assemblies.

Product data

As-Supplied and Cure-Progression Properties

Typical component, mixed-material, and cure-timing data at 22°C unless otherwise stated. Values are representative and are not specifications.

Property Value Unit Method / condition
Product type Two-part toughened methacrylate structural adhesive — Room-temperature-curing adhesive and activator
Mix ratio 1:1 — Adhesive to activator; ratio basis is not stated in the supplied technical data sheet
Viscosity - adhesive 45,000 cP As supplied
Viscosity - activator 40,000 cP As supplied
Mixed viscosity Non-sagging gel — Thixotropic mixed state
Color Off-white — Mixed material
Density - adhesive 1.00 kg/L As supplied
Density - activator 0.97 kg/L As supplied
Mixed density 1.00 kg/L Mixed material
Open time 3 min At 22°C; maximum time after application for surface wetting
Assembly time 6 min At 22°C; mate and position parts before cure progression prevents disturbance
Fixture time 12 min At 22°C; defined by a 1 kg dead weight on a 12.7 mm overlap joint, 25.4 mm wide
Functional cure 1 h At 22°C
Full cure 4 h At 22°C
Coverage 980 cm² per 25 mL At a 0.25 mm applied thickness
Order configuration DS-220 25 mL Dev-Tube Supplied regional technical data sheet
Application

Surface Preparation, Application, and Cure

Clean the adherends, mix the adhesive and activator at the documented 1:1 ratio, apply the mixed material to one surface, and complete part positioning before the 6-minute assembly time expires. Limit thick adhesive masses to control exotherm during the rapid room-temperature cure.

Surface preparation: Solvent-wipe heavy grease, oil, and other contaminants or use suitable industrial cleaning equipment. Abrading or roughening metals increases microscopic bond area.
Mix and application: Mix adhesive and activator 1:1 and apply the mixed adhesive directly to one bonding surface. Prepare only enough material to use within the working time.
Assembly window: Complete application, mating, positioning, and fixturing within the documented assembly time. Do not disturb the parts after cure progression begins.
Gap and exotherm control: Avoid cure thicknesses above 3 mm where possible and confine the applied gap to no more than 3 mm. Large adhesive masses can generate heat and release entrapped air or volatile components.
Substrate boundary: Copper, brass, and aluminum are not recommended in the supplied technical data sheet.
Application visual showing mixed Devcon Plastic Welder placed on a prepared plastic-to-steel joint before assembly

Insert an approved technical image showing surface preparation, controlled adhesive application, or timely mating of a supported dissimilar-substrate joint.

Stage 1
Clean and prepare the adherends
Remove heavy grease, oil, and contaminants. Abrade or roughen metal surfaces when increased microscopic bond area is needed.
Stage 2
Mix and apply
Mix the two components 1:1, prepare only the amount needed within the working time, and apply the mixed adhesive directly to one surface.
Stage 3
Mate, fixture, and cure
Mate and position parts within 6 minutes at 22°C. Plan around the 12-minute fixture time, 1-hour functional cure, and 4-hour full cure.
Storage and Handling

Store Devcon Plastic Welder in its original container in a cool, dry place. The supplied technical data sheet states a shelf life of one year or more at 22°C and notes that refrigeration may extend shelf life. Keep the flammable components away from heat, sparks, and open flames, and consult the current Safety Data Sheet for complete handling, exposure-control, first-aid, storage, and disposal requirements.

Final bonded state

Cured Adhesive Properties

Typical cured adhesive and bonded-joint data. Bond strength is specific to the listed substrate, preparation, and test configuration and should not be treated as a universal design allowable.

Property Value Unit Method / condition
Tensile shear - grit-blasted steel 20.6 MPa ASTM D1002
Tensile shear - polycarbonate alloy 9.6 MPa ASTM D1002; stock failure
Tensile shear - ABS 8.9 MPa ASTM D1002; stock failure
Peel strength 6 kg/cm ASTM D1876
Impact resistance - grit-blasted steel 1.2 kg/m/cm ASTM D950-611; unit reproduced as stated in the source
Hardness 78 Shore D Typical cured material
Minimum elongation 75 % Typical cured material
Operating temperature -20 to 120 °C Supplier also notes intermittent paint-bake exposure above 120°C; duration is not stated
Supported use contexts

Applications

Evaluate the product within the documented substrate list, preparation requirements, 3 mm processing gap limit, cure timing, and operating environment. Copper, brass, and aluminum are not recommended.

Supported mixed-plastic components prepared for bonding with Devcon Plastic Welder
Dissimilar plastic assembly
Bond supported PVC, vinyl, ABS, acrylic, polycarbonate, polystyrene, PET/PETE, and phenolic plastics in combinations suited to the joint design and cure window.
Plastic component positioned on a prepared steel or stainless-steel adherend for structural bonding
Plastic-to-steel structural bonding
Join supported plastics to steel or stainless steel where the surface preparation, assembly timing, load mode, and service exposure align with the documented product data.
Fiberglass, wood, and ceramic parts arranged for a weather- or solvent-exposed mixed-material assembly
Fiberglass, wood, and ceramic assemblies
Use in documented mixed-material bonds involving fiberglass, wood, or ceramics, including assemblies where weather, humidity, temperature variation, or solvent exposure is anticipated.
Next steps

Technical Support

Work with Krayden to evaluate Devcon Plastic Welder against your substrate pair, surface preparation, bond gap, joint geometry, fixture timing, service temperature, weather or solvent exposure, and production process. Our team can help review application trials, dispensing needs, packaging, compatibility boundaries, and implementation requirements.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers