DEVCON PLASTIC STEEL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DEVCON PLASTIC STEEL

Main features

  • Room-Temperature Adhesive Cure
  • 45-Minute Working Window
  • 2,800 psi Cured Tensile Strength

Product Description

Devcon® Plastic Steel Putty (A) is a steel-filled, two-part epoxy putty that cures at room temperature and is designed for filling, rebuilding, and bonding metal surfaces. Its putty consistency supports application on vertical surfaces, and the cured material can be machined to a metallic finish. The product bonds to aluminum, concrete, and many other metals and has a typical 45-minute pot life at 75°F (24°C) with a 16-hour functional cure. After seven days of cure at 75°F (24°C), typical properties include 2,800 psi (19.3 MPa) adhesive tensile shear strength, 8,260 psi (57 MPa) compression strength, and Shore D 85 hardness.

Key features

  • Steel-filled machinable epoxy: Cures at room temperature and can be machined to a metallic finish after cure.
  • Vertical-surface application: Putty consistency and documented application characteristics support filling and rebuilding work on vertical surfaces.
  • Mechanical performance: Typical cured properties include 2,800 psi (19.3 MPa) adhesive tensile shear strength and 8,260 psi (57 MPa) compression strength after seven days at 75°F (24°C).

Applications / Suitable for

  • Patching and repairing areas where welding or brazing would be undesirable or impossible
  • Duplicating or tracing masters
  • Short-run dies and molds
Product Family

DEVCON PLASTIC STEEL

Loading pricing…

Technical Specifications

Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
121 ˚C
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
1.2 kV/mm
Mechanical Properties
Molded Shrinkage
0.0006 %
General Properties
Color
The color
gray
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:5:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
21 minutes
Solids
100 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.33

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and handling properties for product evaluation. Technical data are representative or typical and are not for specification purposes.

Property Value Unit Method / condition
Color Grey — Uncured properties at 72°F (23°C)
Mixed viscosity Putty — Uncured properties at 72°F (23°C)
Mix ratio by volume 2.5:1 — Uncured properties at 72°F (23°C)
Pot life 45 min At 75°F (24°C)
Specific gravity 19.45 (2.33) lb/gal (g/cm³) Uncured properties at 72°F (23°C)
Coverage at 1/4 in. (6.35 mm) 48 (310) in²/lb (cm²/kg) Uncured properties at 72°F (23°C)
Shelf life 3 years From manufacture; store at room temperature, 70°F (21°C)
Technical properties

After-processing / final-state properties

Typical cured-material properties after seven days at 75°F (24°C). Values are representative or typical and are not for specification purposes.

Property Value Unit Method / condition
Adhesive tensile shear 2,800 (19.3) psi (MPa) ASTM D 1002; cured 7 days at 75°F (24°C)
Compression strength 8,260 (57) psi (MPa) ASTM D 695; cured 7 days at 75°F (24°C)
Flexural strength 5,600 (38.6) psi (MPa) ASTM D 790; cured 7 days at 75°F (24°C)
Hardness 85 Shore D ASTM D 2240; cured 7 days at 75°F (24°C)
Cured shrinkage 0.0006 in/in (cm/cm) ASTM D 2566; cured 7 days at 75°F (24°C)
Coefficient of thermal expansion 48 × 10−6 (86.4 × 10−6) in/in·°F (cm/cm·°C) ASTM D 696; cured 7 days at 75°F (24°C)
Temperature resistance Wet: 120 (49); Dry: 250 (121) °F (°C) Typical cured-material temperature resistance
 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers