CYTEC UF-3

Harmonization Code : 3909509090 | Polyurethanes potting

CYTEC UF-3

Main features

  • Two-Component Polyurethane Electronics-Packaging Foam
  • One-Hour Cure Cycle
  • Solvent, Oil, and Moisture Resistance

Product Description

CONATHANE® UF-3 Polyurethane Foam is a two-component liquid polyurethane foam for packaging electronic components and assemblies. The system cures at room temperature or with heat and is documented for low vapor pressure, electrical insulation, and resistance to moisture, oils, grease, and most solvents. Part A is dark amber and Part B is clear, with a 100:90 mix ratio by weight. Typical cure schedules are two to three hours at 25°C or one hour at 60°C, and the cured foam has a documented dielectric strength of 60 V/mil.

Key features

  • Electronic packaging foam: The two-component polyurethane system is documented for packaging electronic components and assemblies.
  • Room-temperature or heat cure: Typical cure schedules are two to three hours at 25°C or one hour at 60°C.
  • Electrical insulation: The cured foam has a documented dielectric strength of 60 V/mil.

Applications / Suitable for

  • Packaging electronic components and assemblies

Technical Specifications

General Properties
Color
The color
Dark Amber / Clear
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Prepolymer / Curative )
Density (g)
7.6 g/cm3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.22 / 1.05
Chemical Properties
Water Absorption
0.6 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color, Part A Dark amber N/A As supplied
Color, Part B Clear N/A As supplied
Viscosity, Part A 200 cP At 25°C
Viscosity, Part B 7,500 cP At 25°C
Specific gravity, Part A 1.22 N/A At 25°C
Specific gravity, Part B 1.05 N/A At 25°C
Mix ratio 100:90 parts by weight Part A : Part B
Cure options 2 to 3 h at 25°C; 1 h at 60°C N/A Typical schedules