CYBERBOND 6001

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 6001

Main features

  • Cyanoacrylate cure acceleration
  • Flexible application methods
  • Ultra-low viscosity

Product Description

Cyberbond Blast 6001 is a cyanoacrylate adhesive accelerator designed to increase the curing speed of Apollo cyanoacrylate adhesives in conditions where low humidity or acidic surfaces may slow bond formation. This colorless, low-viscosity liquid can be applied before or after adhesive placement using a brush, spray, wipe, or dropper. Blast 6001 is commonly used to improve cure speed in gap-filling applications and fillet areas where rapid bond development is beneficial. Its fast-evaporating solvent system supports efficient processing while maintaining application flexibility across a range of assembly operations.

Key features

  • Cyanoacrylate cure acceleration: Speeds the curing of Apollo cyanoacrylate adhesives in low-humidity and surface-acidic environments.
  • Flexible application methods: Can be pre-applied or post-applied using a brush, spray, wipe, or dropper depending on process requirements.
  • Ultra-low viscosity: Approximately 1 cP viscosity supports rapid wetting and easy application to the bonding area.

Applications / Suitable for

  • Accelerating cyanoacrylate adhesive curing.
  • Low-humidity assembly environments.
  • Gap-filling bond applications.
  • Fillet bond conditions.
  • Pre-application or post-application adhesive processes.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.7
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-6.66 to -1.11 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1 mPa.s
Volatiles
100 %
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

Technical properties

As-supplied / before-processing properties

Representative physical properties of Blast 6001 in its supplied liquid form.

Property Value Unit Method / condition
Appearance Colorless liquid — As supplied
Viscosity 1 cP Typical liquid property
Specific Gravity 0.7 — As supplied
Flash Point 20–30 °F Typical value
Shelf Life 12 months Unopened container