CYBERBOND 2010

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2010

Main features

  • 20-Second General-Purpose Fixture
  • Controlled Low-Viscosity Application
  • 2,920 psi Stainless-Steel Shear

Product Description

Cyberbond 2010 is a one-component, solvent-free ethyl cyanoacrylate adhesive for fast general-purpose bonding. It has a typical viscosity of 95 to 200 mPa s at 20 deg C and fixtures in about 20 seconds, supporting controlled application to metals, elastomers, rubber, and plastics. Substrate-specific set times range from 2 to 4 seconds on ABS to 5 to 40 seconds on steel under the stated conditions. The cured adhesive provides a 2,920 psi shear strength on stainless steel and a service temperature range of -55 to 95 deg C.

Key features

  • Fast general-purpose fixture: Typical fixture time is 20 seconds, with substrate-specific set times reported for ABS, EPDM, steel, and beech.
  • Controlled low-viscosity flow: Typical viscosity is 95 to 200 mPa s at 20 deg C using a cone-plate method.
  • Stainless-steel bond strength: Reported cured shear strength is 2,920 psi on stainless steel.

Applications / Suitable for

  • Metal and stainless-steel bonding
  • Elastomer, rubber, and EPDM assemblies
  • Plastic and ABS component bonding

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
85 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
110 +/- 20 mPa.s
Other Properties
Storage Temperature
15.5 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical product and process values. Values are not specifications.

Property Value Unit Method / condition
Physical form Liquid As supplied
Viscosity 95 to 200 mPa s 20 deg C, 158 s^-1, cone-plate method
Density 1.06 g/cm^3 Typical value
Fixture time 20 seconds Typical value
Flash point 82.5 deg C Uncured product

Leading Brands Trust in Our Products and Services