CYBERBOND 2008

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2008

Main features

  • Fast EPDM and Elastomer Bonding
  • Low-Viscosity Close-Fit Wetting
  • Single-Component Rapid Assembly

Product Description

Cyberbond 2008 combines a low-viscosity ethyl cyanoacrylate format with fast bonding for elastomers and plastics. The product is specifically used for EPDM bonding, giving it a focused role where a thin instant adhesive is needed to wet close-fitting rubber interfaces. Its no-mix format supports controlled dispensing and rapid assembly. Cyberbond 2008 is used for small, well-fitted joints where low viscosity and fast set behavior are more important than gap filling. It is intended for fast elastomer and plastic component bonding.

Key features

  • EPDM and elastomer bonding: The adhesive is specifically used for EPDM and other elastomer applications.
  • Low-viscosity interface wetting: The thin liquid format supports close-fitting rubber and plastic joints.
  • Rapid one-part assembly: No resin-to-hardener mixing is required before fast bonding operations.

Applications / Suitable for

  • EPDM component bonding
  • Elastomer and rubber assemblies
  • Close-fitting plastic joints

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
colorless, transparent
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
85 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
10 - 20 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and application characteristics for the one-component adhesive. Values are not specifications.

Property Value Unit Method / condition
Technology / base Ethyl cyanoacrylate One-component adhesive
Physical form Low-viscosity liquid As supplied
Cure mechanism Humidity initiated Cyanoacrylate cure
Primary material context Elastomers and plastics Bonding scope
Specific substrate context EPDM Application material

Leading Brands Trust in Our Products and Services