CYBERBOND 2000

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2000

Main features

  • Low-Viscosity Wicking Bonding
  • Fast Preassembled-Part Fixing
  • Single-Component Drop Dispensing

Product Description

Cyberbond 2000 serves as a one-component ethyl cyanoacrylate wicking adhesive for close-fitting, preassembled parts. Its low-viscosity liquid profile supports capillary flow into narrow interfaces and fast bonding where post-assembly adhesive application is preferred. The product is used for rapid fixture of compatible components without premixing, making it practical for small bond areas and controlled drop dispensing. Cyberbond 2000 suits assembly operations that need an instant adhesive to penetrate tight joints rather than fill gaps.

Key features

  • Low-viscosity wicking flow: The adhesive penetrates close-fitting interfaces in preassembled parts.
  • Fast post-assembly bonding: The cyanoacrylate format supports rapid fixture after the joint is assembled.
  • Single-component dispensing: The liquid is applied without mixing for controlled drop or capillary application.

Applications / Suitable for

  • Preassembled close-fitting parts
  • Narrow interfaces requiring wicking application
  • Small bond areas and rapid fixture operations

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.06
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2 +/- 1 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
85 °C
Operating Temperature
-55 to 95 °C
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and application characteristics for the one-component adhesive. Values are not specifications.

Property Value Unit Method / condition
Technology / base Ethyl cyanoacrylate One-component adhesive
Physical form Low-viscosity liquid As supplied
Cure mechanism Humidity initiated Cyanoacrylate cure
Application behavior Wicking / capillary flow Applied to preassembled parts
Joint fit Close fitting Small clearances

Leading Brands Trust in Our Products and Services