COOLTHERM SC-6711

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6711

Main features

  • 1.0 W/(m K) Thermal Encapsulation
  • 30,000 cP White Silicone Resin
  • 19.7 kV/mm Dielectric Strength

Product Description

CoolTherm® SC-6711 WHT Silicone Encapsulant is a white thermally conductive silicone resin formulated for use with CoolTherm® SC-6731, CoolTherm® SC-6730, or Circalok™ 6732 hardener. The resin has a typical 30,000 cP viscosity at 25°C and 2.2 specific gravity. Hardener selection changes the resin-to-hardener ratio, working life, and room-temperature cure schedule. Supported combinations range from 100:0.5 to 100:5 by weight, with working lives from less than 0.5 hour to 2–3 hours at 25°C and room-temperature cures from 6–8 hours to 12–16 hours. Typical cured properties, stated as common across the supported hardeners, include 1.0 W/m·K thermal conductivity, 60 Shore A hardness, 19.7 kV/mm dielectric strength, and 1 × 1014 ohm-cm volume resistivity.

Key features

  • White thermally conductive silicone resin for two-component encapsulation
  • Compatible with SC-6731, SC-6730, and Circalok™ 6732 hardeners
  • 30,000 cP resin viscosity for pouring, cartridge, or meter/mix/dispense processing
  • Hardener-dependent working life and room-temperature cure control
  • Typical 1.0 W/m·K thermal conductivity and 19.7 kV/mm dielectric strength
  • Low-CTE positioning for severe temperature-cycling designs
  • Flexible 60 Shore A cured silicone with 70% elongation

Applications

  • Thermally conductive electrical and electronic potting
  • Assemblies requiring rapid heat transfer and flexible silicone encapsulation
  • High-temperature electronic applications requiring validated material compatibility
  • Critical or high-voltage assemblies using validated vacuum-assisted void control

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White Paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.2
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
30000 mPa.s
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.0 W/m.K
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
70 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
19.7 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1 x 10^14 Ohms⋅cm

Additional Information

Configurable thermally conductive silicone resin platform

CoolTherm® SC-6711 WHT Silicone Encapsulant

SC-6711 WHT is a white thermally conductive silicone resin that becomes a two-component encapsulant when combined with SC-6731, SC-6730, or Circalok™ 6732 hardener. The hardener choice controls mix ratio, working life, and room-temperature cure while the published cured-property set remains common across the supported combinations.

White silicone resin30,000 cPThree hardener options1.0 W/m·K60 Shore A
CoolTherm SC-6711 WHT silicone resin with compatible hardener packaging

CoolTherm SC-6711 WHT silicone resin with compatible hardener packaging

As supplied

SC-6711 WHT resin properties

Property Typical value Context
Appearance White paste Resin before hardener addition.
Viscosity at 25°C 30,000 cP Resin-only value.
Specific gravity 2.2 Typical resin value.
Hardener selection and processing

Select the hardener first, then meter, mix, minimise air, apply, and cure

Thoroughly remix SC-6711 WHT in its shipping container, weigh the required resin quantity, add the selected hardener at its documented usage level, and mix thoroughly. SC-6730 is blue-green to support visual confirmation of mixing. Use direct pouring, handheld cartridges, or automatic meter/mix/dispense equipment, and complete encapsulation within the applicable working life.

  • Minimise bubbles and voids; vacuuming may be appropriate for extremely high-voltage or critical applications.
  • Avoid high humidity during cure.
  • Do not interchange hardener ratios or cure schedules.
SC-6711 WHT process showing resin remixing, hardener selection, weight metering, mixing, vacuum de-airing, dispensing and room-temperature cure

SC-6711 WHT process showing resin remixing, hardener selection, weight metering, mixing, vacuum de-airing, dispensing and room-temperature cure.

Hardener Resin:hardener by weight Working life at 25°C Cure at 25°C
CoolTherm SC-6731 100:0.5 1–2 hours 12–16 hours
CoolTherm SC-6730 100:3 2–3 hours 12–16 hours
CoolTherm SC-6730 100:5 0.5–1 hour 8–12 hours
Circalok™ 6732 100:0.5 Less than 0.5 hour 6–8 hours

Storage and industrial handling

SC-6711 WHT resin has a six-month shelf life when stored at 25°C in its original unopened container. The supplied EHS identifier did not resolve to readable product-specific safety content. Final publication and use therefore require the current regional resin SDS, the selected hardener SDS, and product labels. Use trained industrial personnel and the required ventilation, personal protection, spill, storage, and waste controls.

Final cured state

Thermal, mechanical, dimensional, and electrical properties

DS3572 states that the following typical cured properties are the same regardless of the supported hardener used. They are bulk-material values, not finished-assembly thermal resistance or working-voltage ratings.

Property Typical value Context
Thermal conductivity 1.0 W/m·K Hot Disc Transient Method, ISO 22007-2.
Coefficient of linear thermal expansion 150 ppm/°C ASTM D696.
Hardness 60 Shore A Flexible cured silicone.
Tensile strength at 25°C 5.51 MPa (800 psi) Typical bulk-material result.
Elongation at break 70% Typical cured-material value.
Volume resistivity at 25°C 1 × 1014 ohm-cm Bulk electrical property.
Dielectric strength 19.7 kV/mm (500 V/mil) Breakdown property, not design working voltage.
Dielectric constant 5.2 Frequency and conditioning not stated in DS3572.
Dissipation factor 0.02 Frequency and conditioning not stated in DS3572.
Applications and design considerations

Flexible thermal encapsulation with hardener-controlled processing

SC-6711 WHT is directly positioned for potting applications requiring rapid heat transfer, high-temperature service, and a flexible silicone system. Final selection must account for the chosen hardener, exact ratio, working life, humidity during cure, fill depth, void tolerance, voltage, thermal path, interfaces, repairability, and environmental exposure.

Product resource

Potting & Encapsulation Materials Catalogue — PC3002

PC3002 lists the SC-6711 WHT/6731 combination at 100:0.5 by weight, 12–16 hours at 25°C, 60 Shore A, 19.7 kV/mm dielectric strength, and 1.0 W/m·K thermal conductivity. The catalogue does not replace DS3572 for the SC-6730 or Circalok 6732 configurations.

Open PC3002

Validate the SC-6711 WHT hardener configuration

Krayden can help review hardener selection, weight-ratio control, working life, humidity, vacuum processing, fill geometry, room-temperature cure, thermal path, electrical insulation, and assembly-level qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services