Main features

  • 1.1 W/(m K) Thermal Interface
  • 1 to 6 mil Spray Coats
  • 59 kV/mm Dielectric Strength

Product Description

CoolTherm® EP-343 Thermally Conductive Epoxy Conformal Coating is a two-component, dielectric epoxy coating recommended for printed circuit boards, semiconductors, and heat sink assemblies. The black, low-viscosity mixed material can be applied with conventional spray equipment at 1–6 mils per application. After the documented cure schedule, it provides a typical thermal conductivity of 1.1 W/m·K, high electrical insulation, and an operating temperature range of -65 to 130 °C. The cured coating also provides resistance to water and a variety of chemicals, along with edge coverage and hiding power in thin applications.

Key features

  • Thermally conductive dielectric coating: Provides a typical cured thermal conductivity of 1.1 W/m·K using the Hot Disc Transient Method, ISO 22007-2.
  • Low-viscosity spray application: The mixed material has a typical viscosity of 55 cP at 25 °C and can be sprayed at 1–6 mils per application.
  • Electrical and temperature performance: Provides a typical dielectric strength of 59 kV/mm at 0.003-inch thickness and supports operating temperatures from -65 to 130 °C.

Applications / Suitable for

  • Printed circuit board coating
  • Semiconductor coating
  • Heat sink assembly coating

:contentReference[oaicite:0]{index=0}

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Resin: Black Liquid | Hardener: Amber Liquid | Mixed: Black Liquid
Physical Properties
Viscosity (Part A)
(Resin) 65 mPa.s
Viscosity (Part B)
(Hardener) 55 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
106 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.1 W/m.K
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
at break 1.9 %
Chemical Properties
Moisture absorption
10 days at 25°C 0.2 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
59 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1 x 10^16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed coating before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid / amber liquid / black liquid — EP-343 resin / EP-343 hardener / mixed material
Mix ratio 100:3.9 By weight EP-343 resin : EP-343 hardener; no dilution required
Viscosity 65 / 55 / 55 cP Resin / hardener / mixed material at 25 °C; test method not stated
Specific gravity 1.41 / 0.99 / 1.35 — Resin / hardener / mixed material; test conditions not stated
Working life 24 hours Mixed material at 25 °C
Recommended applied thickness 1–6 mil Spray-applied in one application; greater thicknesses require partial oven curing between coats
Shelf life 1 / 2 years Resin / hardener when stored at 25 °C in original, unopened containers

 

Technical properties

After-processing / final-state properties

Typical cured properties after an initial cure of 2 hours at 65 °C followed by a post-cure of 4 hours at 135 °C. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 1.1 W/m·K Hot Disc Transient Method, ISO 22007-2
Coefficient of linear thermal expansion 24 ppm/°C ASTM C864
Glass transition temperature 106 °C Test method not stated
Hardness 90 Shore D Test method not stated
Tensile strength 57.22 (8,300) MPa (psi) Test method not stated
Moisture absorption 0.2 % 10 days at 25 °C; exposure medium not stated
Volume resistivity 1 × 1016 ohm-cm ASTM D257 at 25 °C
Dielectric strength 59 (1,500) kV/mm (V/mil) 0.003-inch specimen thickness; ASTM D149

 