COOLTHERM 6053

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM 6053

Main features

  • Flexible Cured Material
  • Heat & Oxidation Resistance
  • Supplied in a 16-Ounce Aerosol Format

Product Description

Circalok™ 6053 Mold Release Agent is an aerosol-applied mold release formulation based on organic and silicone polymers. Formerly identified as EMR-1023, it is intended to release epoxy, polyester, synthetic rubber, and flexible or rigid urethane molding compounds, including TDI- and MDI-based urethane elastomers and polyether or polyester urethane foams. The formulation is described as heat resistant, oxidation resistant, and capable of forming a high-strength release film that helps protect mold surfaces and limit mold buildup. Circalok 6053 is supplied in 16-ounce aerosol cans for direct application to molding tools.

Key features

  • Broad molding-compound coverage: Supports release of epoxy, polyester, synthetic rubber, urethane elastomers, and flexible or rigid urethane foams.
  • Heat- and oxidation-resistant release film: Combines documented heat resistance, oxidation resistance, and high film strength.
  • Aerosol application format: Supplied in 16-ounce aerosol cans for application to mold surfaces.

Applications / Suitable for

  • Reaction injection molding
  • Direct injection molding
  • Casting and transfer molding
  • Potting and laminating processes
Product Family

COOLTHERM 6053

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Organic and silicone polymers
Product Type
Material category or functional product class.
Aerosol

Additional Information

Technical properties

As-supplied / before-processing properties

Supported product identity, formulation, and supply-format information before application to the mold surface.

Property Value Unit Method / condition
Product type Mold release agent — Aerosol-applied formulation
Formulation Organic and silicone polymers — General formulation description
Package format 16 ounce aerosol can Available supply format stated in DS3713