Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-9

Main features

  • Fixed En-4 Plus En-9 System
  • 120-Minute Gel Window
  • Multiple Elevated-Temperature Cures

Product Description

CONATHANE EN-4 / EN-9 is the curative in the fixed EN-4 Part A plus EN-9 Part B polyurethane system. EN-4 Part A is supplied separately and is always required for system use. The mixed and cured values shown apply only to this fixed pair and do not describe EN-9 Part B by itself or a prepacked kit. Documented applications include cables and connectors, modules and wound devices, and printed-circuit coatings. Mix each component before combining.

Key features

  • Material system: Fixed EN-4 plus EN-9 system.
  • Key characteristic: 80 and 120 minute gel points.
  • Processing window: Multiple elevated-temperature cures.

Applications

  • Cables and connectors
  • Modules and wound devices
  • Printed-circuit coatings

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent Amber / Amber
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Urethane Prepolymer / Curative)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100: 17.5
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.97 / 1.00

Additional Information

Potting, encapsulants and underfills

CONATHANE® EN-9 Curative for the EN-4 polyurethane system

CONATHANE® EN-9 is the Part B Curative used with CONATHANE® EN-4 Part A Urethane Prepolymer to form an unfilled, two-component, 100%-solids polyurethane system. The EN-4 plus EN-9 system provides an extended viscosity-development window, reaching 100,000 cP after 80 minutes and 250,000 cP after 120 minutes at 25°C. Mixed, processing, and cured values apply to the complete EN-4 plus EN-9 system and do not describe EN-9 Part B alone.

EN-9 Part B Curative Requires EN-4 Part A 100:17.5 by weight 80 / 120 min viscosity endpoints Non-MbOCA system

Technical properties

EN-9 Part B as-supplied properties

Property Value Unit Method / condition
Appearance Amber Not applicable As supplied
Viscosity 950 cP 25°C / 77°F
Specific gravity 1.00 Unitless 25°C / 77°F

EN-4 plus EN-9 system

Component and mixed-material properties

Property State / condition Typical value Unit
EN-4 Part A viscosity 25°C / 77°F 7,500 cP
EN-4 Part A specific gravity 25°C / 77°F 0.97 Unitless
Mix ratio EN-4 : EN-9 By weight 100:17.5 Parts
Mix ratio EN-4 : EN-9 By volume 100:17 Parts
Initial mixed viscosity 25°C / 77°F 6,800 cP
Gel time 100,000 cP at 25°C 80 min
Gel time 250,000 cP at 25°C 120 min
Peak exotherm 2 lb mass at 25°C 55 / 130 °C / °F

Data scope: The EN-4 Part A value shown here is the value stated in the EN-9 system TDS. Mixed values apply only to the EN-4 plus EN-9 system.

Processing

Mix, degas, cure, and demold

Prepare and combine

Mix individual components before combining. Use 100 parts EN-4 Part A with 17.5 parts EN-9 Part B by weight, or 100:17 by volume, and mix until homogeneous.

Preheat and degas

Components may be preheated up to 60°C when reduced viscosity is required. For hand mixing, degas at greater than 27 in. Hg vacuum before use.

Application methods

Supported methods include hand-mix bench potting or casting, meter-mix bench potting or casting, and meter-mix vacuum potting or casting.

Stage Temperature Time
Cure 60°C / 140°F 24 h
Cure 80°C / 176°F 16 h
Cure 100°C / 212°F 8 h
Demold 60°C / 140°F 10 h
Demold 80°C / 176°F 8 h
Demold 100°C / 212°F 4 h

Processing boundary: Cure and demold timing begins after the unit reaches the stated temperature. The schedules are recommendations and should be evaluated for the actual application.

Cured EN-4 plus EN-9 system

Typical mechanical and environmental properties

Property Method Condition Typical value Unit
Specific gravity ASTM D792 25°C 1.01 Unitless
Shore hardness ASTM D2240 25°C A 90 Shore A
Shore hardness ASTM D2240 After 7 d at 135°C A 98 Shore A
Tensile strength ASTM D412 25°C 2,000 psi
100% modulus ASTM D412 25°C 700 psi
300% modulus ASTM D412 25°C 1,300 psi
Ultimate elongation ASTM D412 25°C 450 %
Tear strength ASTM D624 25°C 280 pli
Linear shrinkage MIL-M-24041C Cured 1 %
Volumetric shrinkage MIL-M-24041C Cured 4 %
Moisture absorption MIL-M-24041C 24 h at 93°C 0.5 %
Water absorption ASTM D570 24 h / 30 d at 25°C 0.2 / 0.4 %
Heat-aging weight loss MIL-M-24041C 7 d at 135°C 0.5 %
Fungus resistance MIL-E-5272C Cured system Non-nutrient Result
Thermal shock MIL-I-16923E -70°C to 130°C Pass, 10 cycles Result
Compression set ASTM D395 Method B 44 %

Electrical performance

Typical EN-4 plus EN-9 electrical properties

Property Method Condition Typical value Unit
Dielectric strength ASTM D149 1/16 in at 25°C 750 V/mil
Dielectric constant ASTM D150 100 Hz / 1 kHz / 1 MHz at 25°C 3.0 / 2.9 / 2.8 Unitless
Dielectric constant ASTM D150 100 Hz / 1 kHz / 1 MHz at 130°C 3.8 / 3.8 / 3.3 Unitless
Dissipation factor ASTM D150 100 Hz / 1 kHz / 1 MHz at 25°C 0.03 / 0.03 / 0.01 Unitless
Dissipation factor ASTM D150 100 Hz / 1 kHz / 1 MHz at 130°C 0.03 / 0.03 / 0.04 Unitless
Volume resistivity ASTM D257 25°C / 130°C >4.3 x 1015 / 7.4 x 1011 ohm-cm
Surface resistivity ASTM D257 25°C / 130°C >1.0 x 1015 / 1.6 x 1012 ohms/sq.
Insulation resistance MIL-M-24041C 25°C / 130°C >2.5 x 1013 / 2.3 x 1010 ohms
Arc resistance MIL-M-24041C 25°C 120 seconds
Flame resistance MIL-M-24041C 55 amps DC No ignition Result

Hydrolytic stability

112-day exposure at 97°C / 95% RH

Property Original After 112 days Unit
Shore hardness A 90 A 87 Shore A
Tensile strength 2,000 1,700 psi
300% modulus 775 700 psi
Ultimate elongation 450 370 %
Tear strength, Die C 280 190 pli
Dielectric strength 750 570 V/mil
Dielectric constant, 1 kHz 2.9 3.0 Unitless
Dissipation factor, 1 kHz 0.03 0.03 Unitless
Volume resistivity 4.3 x 1015 2.8 x 1015 ohm-cm

Data scope: Values are typical and are not intended for specification use.

Applications

Applications for the EN-4 plus EN-9 system

Cables and connectors

Potting and molding of military and commercial cables and connectors, watertight electrical connectors, harness breakouts, and cables.

Modules and wound devices

Potting and encapsulation of modules, wire-wound devices, and strain-sensitive components.

Printed circuitry

100%-solids and solvent-based coating applications for printed circuitry and components.

Storage and handling

Protect EN-9 and EN-4 from moisture

Store below 25°C / 77°F in a dry controlled environment away from direct sunlight. The stated shelf life is 12 months from shipment in the original sealed containers under the specified storage conditions.

The components are sensitive to moisture and atmospheric humidity. Protect opened material with dry air or nitrogen before resealing. If EN-4 Part A crystallizes during storage or shipment, heat it to 60°C, mix thoroughly, and cool to room temperature before processing.

Discuss EN-9 with EN-4 Part A

Krayden can help evaluate the EN-4 plus EN-9 system around its extended viscosity-development window, cure temperature, demold requirement, mechanical and electrical properties, assembly geometry, and service environment.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers