CONATHANE EN-7

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-7

Main features

  • Fixed En-4 Plus En-7 System
  • 30-Minute Gel Window
  • Multiple Cure Schedule Options

Product Description

CONATHANE EN-4 / EN-7 is the curative in the fixed EN-4 Part A plus EN-7 Part B polyurethane system. EN-4 Part A is supplied separately and is always required for system use. The mixed and cured values shown apply only to this fixed pair and do not describe EN-7 Part B by itself or a prepacked kit. Documented applications include cables and connectors, modules and wound devices, and printed-circuit coatings. Cure options are 10 to 14 days at 25 C, 16 hours at 60 C, 8 to 10 hours at 80 C, or 4 to 6 hours at 100 C.

Key features

  • Material system: Fixed EN-4 plus EN-7 system.
  • Processing window: 30-minute typical gel time.
  • System options: Multiple cure schedule options.

Applications

  • Cables and connectors
  • Modules and wound devices
  • Printed-circuit coatings

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent Amber / Amber
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Urethane Prepolymer / Curative)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100: 17.5
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.97 / 1.00
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>94 °C

Additional Information

Potting, encapsulants and underfills

CONATHANE® EN-7 Curative for the EN-4 polyurethane system

CONATHANE® EN-7 is the Part B Curative used with CONATHANE® EN-4 Part A Urethane Prepolymer to form an unfilled, two-component, room-temperature-curing, 100%-solids polyurethane system. The complete EN-4 plus EN-7 system is used for electrical and electronic potting, molding, encapsulation, and selected coating applications. Mixed and cured values apply to the complete system and do not describe EN-7 Part B alone.

EN-7 Part B Curative Requires EN-4 Part A 100:17.5 by weight 30 min gel time Non-MbOCA system

Technical properties

EN-7 Part B as-supplied properties

These values describe EN-7 Part B before mixing with EN-4 Part A.

Property Value Unit Method / condition
Appearance Amber Not applicable As supplied
Viscosity 1,000 cP 25°C / 77°F
Specific gravity 1.00 Unitless 25°C / 77°F
Flash point >94 / >201 °C / °F ASTM D93

EN-4 plus EN-7 system

Mix ratio and mixed-material properties

Property Condition Typical value Unit
Mix ratio EN-4 : EN-7 By weight 100:17.5 Parts
Mix ratio EN-4 : EN-7 By volume 100:17 Parts
Initial mixed viscosity 25°C / 77°F 5,500 cP
Gel time 25°C / 77°F 30 min
Peak exotherm 2 lb mass at 25°C / 77°F 55 / 130 °C / °F

Processing

Mix, degas, cure, and demold

Prepare and combine

Mix individual components before combining. Mix 100 parts EN-4 Part A with 17.5 parts EN-7 Part B by weight, or 100:17 by volume, until homogeneous.

Preheat and degas

Components may be preheated up to 60°C when reduced viscosity is required. For hand mixing, degas the mixed material at greater than 27 in. Hg vacuum before use.

Application methods

Supported methods include hand-mix bench potting or casting, meter-mix bench potting or casting, and meter-mix vacuum potting or casting.

Stage Temperature Time
Cure 25°C / 77°F 10 to 14 d
Cure 60°C / 140°F 16 h
Cure 80°C / 176°F 8 to 10 h
Cure 100°C / 212°F 4 to 6 h
Demold 25°C / 77°F 8 h
Demold 60°C / 140°F 3 h

Processing boundary: Cure timing begins after the unit reaches the specified temperature. Cure schedules are recommendations and should be evaluated for the actual application.

Cured EN-4 plus EN-7 system

Typical mechanical and environmental properties

Property Method Condition Typical value Unit
Specific gravity ASTM D792 25°C 1.01 Unitless
Shore hardness ASTM D2240 25°C A 90 Shore A
Tensile strength ASTM D412 25°C >2,000 psi
Ultimate elongation ASTM D412 25°C >400 %
Tear strength ASTM D624 25°C >200 pli
Linear shrinkage MIL-M-24041C Cured 1.2 %
Volumetric shrinkage MIL-M-24041C Cured 3.7 %
Water absorption ASTM D570 24 h at 25°C 0.2 %
Water absorption ASTM D570 30 d at 25°C 0.4 %
Thermal shock MIL-I-16923E -70°C to 130°C Pass, 10 cycles Result

Electrical performance

Typical cured-system electrical properties

Property Method Condition Typical value Unit
Dielectric strength ASTM D149 1/16 in at 25°C 780 V/mil
Dielectric constant ASTM D150 100 Hz / 1 kHz / 1 MHz at 25°C 3.0 / 2.9 / 2.8 Unitless
Dielectric constant ASTM D150 100 Hz / 1 kHz / 1 MHz at 130°C 3.8 / 3.8 / 3.3 Unitless
Dissipation factor ASTM D150 100 Hz / 1 kHz / 1 MHz at 25°C 0.03 / 0.03 / 0.03 Unitless
Volume resistivity ASTM D257 25°C / 130°C >4.3 x 1015 / 7.4 x 1011 ohm-cm
Surface resistivity ASTM D257 25°C / 130°C >1.0 x 1015 / 1.6 x 1012 ohms/sq.
Insulation resistance MIL-M-24041C 25°C / 130°C >2.5 x 1013 / 2.3 x 1010 ohms
Arc resistance MIL-M-24041C 25°C >120 seconds

Hydrolytic stability

112-day exposure at 97°C / 95% RH

Property Original After 112 days Unit
Shore hardness A 94 A 87 Shore A
Tensile strength 2,250 1,750 psi
Ultimate elongation 400 370 %
Tear strength, Die C 320 190 pli
Dielectric strength 780 570 V/mil
Volume resistivity >4.2 x 1015 2.8 x 1015 ohm-cm

Data scope: Values are typical and are not intended for specification use.

Applications

Applications for the EN-4 plus EN-7 system

Cables and connectors

Potting and molding of military and commercial cables and connectors, watertight electrical connectors, harness breakouts, and cables.

Modules and wound devices

Potting and encapsulation of modules, wire-wound devices, and strain-sensitive components.

Printed circuitry

100%-solids and solvent-based coating applications for printed circuitry and components.

Storage and handling

Protect the system components from moisture

Store at or below 25°C / 77°F in a dry controlled environment away from direct sunlight. The stated shelf life is 12 months from shipment in original sealed containers under the specified storage conditions.

The components are sensitive to moisture and atmospheric humidity. Protect opened material with dry air or nitrogen before resealing. If EN-4 Part A crystallizes during storage or shipment, heat to 60°C, mix thoroughly, and cool to room temperature before processing.

Discuss EN-7 with EN-4 Part A

Krayden can help evaluate the EN-4 plus EN-7 system around the required mixed viscosity, 30-minute gel time, cure schedule, demold target, electrical requirements, assembly geometry, and service environment.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers