CONATHANE EN-5310

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-5310

Main features

  • Re-Enterable Polyurethane System
  • 1:1 Controlled Mixing
  • 3,000 cP Mixed Viscosity

Product Description

CONATHANE EN-5310 is a two-component, unfilled polyurethane potting compound for re-enterable electrical and electronic encapsulation. It offers a 1:1 volume mix option, a typical 3,000 cP initial mixed viscosity at 25 C, a 10 to 20 minute work life, and ratio-dependent cured properties. Combine the selected quantities and mix until homogeneous. Listed cured configurations span 17 to 55 Shore A hardness, 240 to 550 psi tensile strength, and 85% to 170% elongation.

Key features

  • Material system: Re-enterable polyurethane system.
  • Key characteristic: 1:1 volume mix option.
  • Flow and dispensing: 3,000 cP mixed viscosity.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
amber / light amber or black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Urethane Prepolymer / Curative)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.14 / 0.97
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
> 94 °C

Additional Information

Potting, encapsulants and underfills

CONATHANE EN-5310 re-enterable potting system

CONATHANE EN-5310, formerly CONATHANE DPEN-22400, is a two-component, unfilled polyurethane potting compound for re-enterable electrical and electronic encapsulation. It offers a 1:1 volume mix option, a typical 3,000 cP initial mixed viscosity at 25 C, a 10 to 20 minute work life, and ratio-dependent cured properties.

Two-componentRe-enterable1:1 volume option3,000 cP mixed

Selection data

As-supplied and mixed properties

Component and mixed values are identified by material state and reported at 25 C unless another condition is shown.

Property State Condition Typical value Unit
Viscosity Part A 25 C 8,100 cP
Viscosity Part B 25 C 350 cP
Specific gravity Part A 25 C 1.14 Unitless
Specific gravity Part B 25 C 0.97 Unitless
Appearance Part A As supplied Amber Not applicable
Appearance Part B As supplied Light amber or black Not applicable
Flash point Part A and Part B ASTM D93 >94 C
Initial viscosity Mixed system 25 C 3,000 cP
Work life Mixed system 25 C 10 to 20 min

Data scope:Values are typical, not specification limits. The selected Part A:Part B ratio controls the cured-property profile.

Processing

Mix, degas, and cure

Select one Part A:Part B ratio and keep that configuration consistent through mixing, degassing, cure, and final-property interpretation.

Select and prepare

Use the Part A:Part B ratio chosen for the required cured-property profile. Mix components in metal or glass equipment and avoid introducing moisture.

Mix and degas

Combine the selected quantities and mix until homogeneous. Degas the mixed system at more than 27 in Hg vacuum at room temperature, leaving capacity for material froth.

Place and cure

Pour or dispense into the prepared assembly. The room-temperature cure recommendation is 5 to 7 days at 25 C.

Processing boundary:EN-5310 supports multiple Part A:Part B ratios. Keep the selected ratio, cure schedule, and matching cured-property row together for the actual assembly.

Storage and handling

Protect components from moisture

Store Part A and Part B at or below 25 C in a dry location away from sunlight. Shelf life is 12 months from shipment in original sealed containers. Both components are moisture-sensitive. If Part A crystallizes, heat it to 60 C, mix until uniform, and cool before use.

Cured system

Ratio-dependent final properties

Each row is one exact Part A:Part B configuration for the cured EN-5310 system. Values must be selected from a single row.

A:B by weight A:B by volume Shore A Tensile strength (psi) Elongation (%) Tear strength (pli) Water absorption 24 h (%) Water absorption 7 d (%) Dielectric strength (V/mil)
100:140 100:165 17 240 170 13.6 0.60 0.83 490
100:126 100:150 30 360 140 18.5 0.56 0.80 510
100:110 100:130 45 390 90 21.5 0.55 0.79 500
100:80 100:94 55 550 85 19.2 0.49 0.74 500

Data scope:Typical cured values at 25 C are ratio-dependent and are not specifications. Do not interpolate or combine data across ratio rows.

Applications

Re-enterable electrical and electronic encapsulation

EN-5310 is used for potting and encapsulating electrical and electronic assemblies where a re-enterable polyurethane system is required. Select the Part A:Part B ratio around the assembly geometry, desired hardness, tensile and elongation profile, processing window, and expected re-entry needs.

Select an EN-5310 configuration

Krayden can help select an EN-5310 Part A:Part B configuration for the target assembly. Share the geometry, desired re-entry behavior, hardness, tensile and elongation priorities, dispensing method, batch mass, work window, and cure conditions so the ratio, processing sequence, and cured-property targets can be evaluated together.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers