CONATHANE EN-2523

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-2523

Main features

  • Filled Polyurethane Electrical Encapsulant
  • 2,800 cP Mixed Viscosity
  • 50% Cured Elongation

Product Description

CONATHANE® EN-2523 Polyurethane Encapsulant is a black, two-component, filled polyurethane casting and encapsulation system for electrical and electronic assemblies exposed to extreme environments and thermal shock. The mixed material has a typical viscosity of 2,800 cP at 25°C and a 50-minute working time, supporting potting processes that require flow around components before cure. The system may cure at room temperature or with heat and is documented for resistance to salt water, aliphatic hydrocarbons, mild acids, and mild bases. Typical cured properties include Shore D 50 hardness, 50% elongation, and electrical insulation.

Key features

  • Filled polyurethane system: The black two-component material is formulated for potting electrical and electronic devices.
  • Controlled processing window: Typical mixed viscosity is 2,800 cP with a 50-minute working time at 25°C.
  • Environmental resistance: The cured system is documented for thermal shock and exposure to salt water, aliphatic hydrocarbons, mild acids, and mild bases.

Applications / Suitable for

  • Electrical and electronic devices exposed to thermal shock
  • Potting assemblies used in adverse environments
  • Room-temperature or heat-cured polyurethane encapsulation

Technical Specifications

General Properties
Color
The color
Brown / Tan or Black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Urethane Prepolymer / Curative)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.24 / 1.46
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.83 hours
Electrical Properties
Arc Resistance
ASTM-D495 expresses arc resistance as the number of seconds that a material resists forming a surface-conducting path when exposed to a high-voltage, low-current arc occurring intermittently. Results obtained from a nominal 3 mm thickness are meant to represent the material’s reaction in any thickness.
130 s
Surface Resistivity
1.5 x 10¹³ Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
3.4 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color Black N/A As supplied
Components Two-part N/A System configuration
Mixed viscosity 2,800 cP At 25°C
Mixed specific gravity 1.44 N/A At 25°C
Working time 50 min At 25°C
Cure options 7 days at 25°C; 16 h at 80°C N/A Documented schedules
Flash point, Part A 199 °C As supplied
Flash point, Part B >100 °C As supplied
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 50 Shore D Typical cured value
Tensile strength 1,600 psi Typical cured value
Elongation 50 % Typical cured value
Dielectric strength >400 V/mil Typical cured value
Volume resistivity 3.4 × 10¹³ ohm·cm At 25°C