CONATHANE CE-1155

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONATHANE CE-1155

Main features

  • Two-Component Polyurethane Conformal Coating
  • Six-Hour Working Window
  • Spray, Dip, or Brush Application

Product Description

CONATHANE CE-1155 is a two-component, solvent-based polyurethane conformal coating for printed circuit boards and electronic assemblies. The system can be applied by spray, dip, or brush. It mixes at 100:70 by weight, has a documented 6-hour pot life for a 400 g mass at 25 deg C, and includes a fluorescent dye to support ultraviolet inspection of the applied film. Documented applications include printed circuit boards, microelectronics, and controller units and electrical devices.

Key features

  • Material system: Two-component solvent-based polyurethane conformal coating for printed circuit boards and electronic assemblies.
  • Mix ratio: 100:70 by-weight mix ratio with 72 cP initial mixed viscosity and 6-hour pot life at 25 deg C.
  • Processing window: Spray, dip, or brush application with documented room-temperature and elevated-temperature cure schedules.

Applications

  • Printed circuit boards
  • Microelectronics
  • Controller units and electrical devices

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
2 Part
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
72 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
118 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.2E16 Ohms⋅cm

Additional Information

Conformal Coatings

Two-component polyurethane coating for electronic assemblies

CONATHANE CE-1155 is a two-component, solvent-based polyurethane conformal coating for printed circuit boards and electronic assemblies. The system can be applied by spray, dip, or brush. It mixes at 100:70 by weight, has a documented 6-hour pot life for a 400 g mass at 25 deg C, and includes a fluorescent dye to support ultraviolet inspection of the applied film.

Two-component polyurethane100:70 by weight72 cP initial mixed viscosity6 h pot life at 25 deg CUV-fluorescent inspection

As supplied

Typical Part A and Part B properties

Component properties are separated from mixed and cured coating data.

Property Part A Part B
Color Clear amber Clear amber
Brookfield viscosity at 25 deg C 300 cP 70 cP
Specific gravity at 25 deg C 1.13 0.96
Solids content 60% 64-66%
NCO content 10.2-10.7% Not reported
Flash point, Seta Flash 81 F 45 F
Shelf life at 25 deg C 15 months 15 months

Processing

Mix, adjust viscosity if required, coat, and cure

CE-1155 uses a 100:70 Part A/Part B weight ratio with time-dependent mixed viscosity, defined film-build limits, recoating intervals, and cure schedules.

  1. Mix Part A and Part B thoroughly at 100:70 by weight. Air bubbles introduced during mixing are stated to dissipate in a few minutes.
  2. At 25 deg C, typical Brookfield mixed viscosity is 72 cP initially, 92 cP after 1 hour, 172 cP after 3 hours, and 432 cP after 6 hours.
  3. Apply by spray, dip, or brush. CONAP S-8 solvent may be used to reduce viscosity or adjust film thickness; 10-20% dilution is recommended for most applications.
  4. Limit one wet-film application to 2-2.5 mil to reduce the possibility of solvent entrapment. For multiple coats, allow 2 hours at room temperature or 30 minutes at 60 deg C before recoating.
  5. Documented cure schedules are 5-7 days at 25 deg C, 3 hours at 60 deg C, or 1 hour at 100 deg C, with corresponding tack-free times of 4-5 hours, 30-45 minutes, and 10-15 minutes.

Storage and handling

Maintain sealed storage and protect Part A from low-temperature crystallization

Store CE-1155 at 65-85 F (approximately 18-29 deg C) in tightly closed containers. If a container is partially used, flush it with dry nitrogen or dry air before resealing.

Shelf life is 15 months from date of manufacture in the original unopened containers under the recommended storage conditions.

If Part A crystallizes after low-temperature exposure, heat the container for 2-4 hours at 50-60 deg C until clear, then cool to room temperature before use.

Cured coating

Typical cured film and electrical properties

These values describe the cured CE-1155 film under the stated test conditions.

Property Typical value Condition / method
Color Clear Cured film
Sward rocker hardness 70 Cured film
Pencil hardness HB Cured film
Dielectric constant 3.50 / 3.43 / 3.21 25 deg C at 100 Hz / 1 kHz / 1 MHz
Dissipation factor 0.0142 / 0.0138 / 0.0162 25 deg C at 100 Hz / 1 kHz / 1 MHz
Volume resistivity 1.18 x 10^16 ohm-cm 25 deg C
Surface resistivity 5.66 x 10^14 ohm 25 deg C
Dielectric strength 3000 V/mil / 1045 V/mil 0.002 in film / 0.022 in film

Performance evidence

Insulation resistance during humidity cycling

For a 1.5-2.0 mil film, insulation resistance was recorded through ten humidity cycles. Adhesion to epoxy-glass panels was maintained during the test, and no under-film corrosion of the copper conductors was observed.

Condition Insulation resistance
Initial, 25 deg C / 50% RH >2.5 x 10^13 ohm
1st cycle, 65 deg C / 95% RH 3.7 x 10^11 ohm
4th cycle, 65 deg C / 95% RH 1.4 x 10^11 ohm
7th cycle, 65 deg C / 95% RH 8.8 x 10^10 ohm
10th cycle, 65 deg C / 95% RH 6.1 x 10^10 ohm
24 h after 10th cycle, 25 deg C / 50% RH 6.0 x 10^12 ohm

Dataset applies to the stated film thickness and humidity-cycle conditions.

Applications

Supported applications

Use the documented application scope below as the starting point for product evaluation.

Printed circuit boards

Conformal coating of printed circuit boards by spray, dip, or brush within the documented film-build and cure process.

Microelectronics

Microelectronics coating applications identified for CE-1155 in the supplied ELANTAS product selection material.

Controller units and electrical devices

Controller-unit and electrical-device coating applications identified for CE-1155 in the supplied ELANTAS selection material.

Technical support for CONATHANE CE-1155

Need help evaluating CE-1155 for a printed circuit board, coating method, wet-film build, recoating interval, or cure schedule? Krayden can help review the assembly geometry, application process, film-thickness target, inspection approach, and electrical or environmental test requirements before the coating is evaluated on the intended hardware.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers