CONAPOXY RN-1200

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONAPOXY RN-1200

Main features

  • Undiluted Unfilled Epoxy Resin
  • 10,000 cP Resin Viscosity
  • Selectable CONACURE Hardener Options

Product Description

CONAPOXY RN-1200 Epoxy Resin is an undiluted, unfilled epoxy resin component for electrical and electronic potting and casting systems. Its 10,000 cP viscosity at 25 deg C supports processing where a relatively fluid resin is needed. The resin is used with a separately selected CONACURE hardener, allowing the complete system to be matched to working-life, flexibility and cure requirements. Because the hardener determines the mix ratio, cure schedule and final properties, RN-1200 should be evaluated as the resin component rather than as a complete cured system.

Key features

  • Undiluted Epoxy Resin: provides an unfilled resin base for potting and casting systems
  • 10,000 cP Viscosity: supports relatively fluid processing at 25 deg C
  • Selectable CONACURE Hardeners: allows working life and cured behavior to be matched to the application

Applications

Resin component for electrical and electronic potting or casting systems using a compatible CONACURE hardener.

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
10,000 mPa.s
General Properties
Color
The color
amber
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.16
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
94 °C

Additional Information

POTTING & ENCAPSULATION

CONAPOXY® RN-1200 two-component epoxy potting system

CONAPOXY® RN-1200 is an unfilled, two-component epoxy potting system for potting and encapsulation of electrical and electronic devices such as modules, transformers and coils. The RN-1200 Resin is combined with a selected CONACURE® hardener to provide different processing windows and cured-property profiles.

Two-component epoxy Unfilled system Low exotherm Low shrinkage Thermal shock resistance Multiple curative options

KEY CHARACTERISTICS

Electrical insulation with configurable processing and cured properties

Selecting the hardener changes the RN-1200 system's processing window and final material properties while retaining the same RN-1200 epoxy resin base.

Low exotherm and shrinkage

The unfilled epoxy system is formulated for low exotherm and low shrinkage during potting and casting.

Thermal shock resistance

RN-1200 systems provide thermal shock resistance, with the EA-028 system specifically identified for very good thermal shock resistance.

Electrical insulation

The cured systems provide good electrical properties with very good arc resistance and typical dielectric strength of 350 V/mil.

Flexible curative selection

EA-02, EA-028 and EA-87 provide different pot-life, viscosity, flexibility and cure characteristics for process selection.

SYSTEM SELECTION

Select the CONACURE® hardener for the required process window

RN-1200 Resin can be combined with EA-02, EA-028 or EA-87 Hardener. Each pairing remains a distinct two-component formulation with its own mix ratio and processing characteristics.

Hardener Processing characteristics Pot / work time Mix ratio by weight
RN-1200 : Hardener
Mix ratio by volume
RN-1200 : Hardener
CONACURE® EA-02 Room-temperature cure, low viscosity and rigid castings 30 min work time 100 : 11 100 : 13
CONACURE® EA-028 Limited flexibility, low viscosity, room-temperature thin-film cure and very good thermal shock resistance 30 min pot life 100 : 28 100 : 32
CONACURE® EA-87 Limited flexibility and low viscosity; heat is required to cure thin films 90 min pot life 100 : 37 100 : 45

AS-SUPPLIED PROPERTIES

RN-1200 Resin and compatible hardener properties

Component properties are shown separately before mixing. Viscosity and specific gravity values apply at 25°C / 77°F.

Property RN-1200 Resin EA-02 Hardener EA-028 Hardener EA-87 Hardener
Viscosity at 25°C / 77°F 10,000 cP 55 cP 40 cP 60 cP
Specific gravity at 25°C / 77°F 1.16 0.98 1.00 0.96
Color Amber Amber Amber Light amber
Flash point, ASTM D93 >94°C / >201°F >94°C / >201°F >94°C / >201°F >94°C / >201°F

Values are typical and are not intended for specification use.

MIXED MATERIAL PROPERTIES

Initial viscosity and gel time by hardener

Mixed-system viscosity and gel time vary with the selected hardener. The values below apply at 25°C / 77°F.

Property RN-1200 + EA-02 RN-1200 + EA-028 RN-1200 + EA-87
Initial viscosity 3,000 cP 1,500 cP 1,500 cP
Gel time 30 min 40 min 60 min

Pot life, work time and gel time are separate processing characteristics and should not be treated as interchangeable.

ELECTRICAL PERFORMANCE

Typical cured-system electrical properties

Property Method / condition EA-02 EA-028 EA-87
Dielectric strength ASTM D149, 25°C / 77°F 350 V/mil 350 V/mil 350 V/mil
Dielectric constant ASTM D150, 1 kHz at 25°C 3.5 4.7 5.0
Dissipation factor ASTM D150, 1 kHz at 25°C 0.017 0.001 0.035
Volume resistivity ASTM D257 2.0 × 1014 ohm-cm 4.0 × 1012 ohm-cm 4.2 × 1015 ohm-cm
Surface resistivity ASTM D257 2.4 × 1015 ohms/sq. 1.0 × 1015 ohms/sq. 8.8 × 1015 ohms/sq.

Values are typical and are not intended for specification use.

CURED PHYSICAL PROPERTIES

Mechanical and thermal properties by hardener

Property Method / condition EA-02 EA-028 EA-87
Shore hardness ASTM D2240, 25°C / 77°F D 84 D 84 D 85
Tensile strength ASTM D412, 25°C / 77°F 10,000 psi 7,600 psi 8,100 psi
Compressive strength ASTM D695, 25°C / 77°F 18,000 psi 12,000 psi 13,500 psi
Linear shrinkage MIL-M-24041C, 25°C / 77°F 1.1% 1.2% 0.8%
Glass transition temperature DSC 85°C / 185°F 70°C / 158°F 85°C / 185°F
Coefficient of thermal expansion Typical 55 ppm/°C 55 ppm/°C 55 ppm/°C
Thermal conductivity Typical 0.2 W/m·K 0.2 W/m·K 0.2 W/m·K

Values are typical and are not intended for specification use. Final properties remain specific to the selected RN-1200 / CONACURE® hardener pairing.

PROCESSING

Mixing, viscosity adjustment and degassing

  1. Select EA-02, EA-028 or EA-87 Hardener for the intended RN-1200 formulation.
  2. Mix RN-1200 Resin and the selected hardener at the specified weight or volume ratio until homogeneous.
  3. Components may be preheated up to 60°C when reduced viscosity is required.
  4. For hand mixing, degas the mixed material at greater than 27 in. Hg vacuum before use.

Recommended cure schedule

Room-temperature cure: 24 hours at 25°C / 77°F

Heat cure: 2 hours at 60°C / 140°F

Cure time begins after the unit reaches the specified temperature. Cure schedules are recommendations, and optimum conditions should be established for the specific application.

APPLICATIONS

Potting and encapsulation of electrical and electronic devices

RN-1200 systems are used for potting and encapsulation applications including modules, transformers and coils.

Electrical modules

Potting and encapsulation of electrical and electronic module assemblies.

Transformers

Electrical insulation and encapsulation of transformer assemblies.

Coils

Potting and encapsulation of electrical coil assemblies.

APPLICATION METHODS

Bench and vacuum potting processes

Hand-mix bench potting / casting
Meter-mix bench potting / casting
Meter-mix vacuum potting / casting

STORAGE & HANDLING

Protect components from heat, sunlight and atmospheric moisture

Store at or below 25°C / 77°F in a dry, controlled environment out of direct sunlight.

Under these conditions, material in the original sealed containers should be suitable for use for twelve months from the date of shipment.

Moisture-sensitive handling

The product is sensitive to moisture and atmospheric humidity. Once opened, containers should be used immediately or blanketed with dry air or nitrogen before resealing.

Mix and degas individual components thoroughly before use.

Discuss your RN-1200 application with Krayden

Share your application, processing method, required working time and cured-property priorities to evaluate the appropriate RN-1200 and CONACURE® hardener combination.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers