CONAPOXY RN-1000

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONAPOXY RN-1000

Main features

  • Amber Epoxy Potting and Casting Resin Compatible
  • 24-Hour 25 deg C Cure
  • Three Curing-Agent Systems

Product Description

CONAPOXY® RN-1000 Epoxy Encapsulant Resin is an amber epoxy resin for potting and casting when combined with CONACURE EA-02, EA-028, or EA-87 curing agent. The three documented systems cure at room temperature or with heat and are positioned for epoxy encapsulation where electrical properties, thermal-shock resistance, low exotherm, and low shrinkage are required. The resin has a listed specific gravity of 1.13. Mix ratio, mixed viscosity, Shore D hardness, tensile strength, and volume resistivity vary with the selected curing agent, so the system configuration must remain explicit.

Key features

  • Potting and casting resin: The amber epoxy resin is used with CONACURE EA-02, EA-028, or EA-87.
  • Room-temperature or heat cure: Each documented system cures for 24 hours at 25°C or two hours at 60°C.
  • Hardener-dependent properties: Mix ratio, mixed viscosity, hardness, tensile strength, and volume resistivity vary by curing agent.

Applications / Suitable for

  • Epoxy potting and casting
  • Electrical and electronic encapsulation
  • Systems using CONACURE EA-02, EA-028, or EA-87

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
800 mPa.s
General Properties
Color
The color
amber
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.14

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin color Amber N/A As supplied
Resin specific gravity 1.13 N/A As supplied
Mix ratio with EA-02 100:11 parts by weight Resin : curing agent
Mixed viscosity with EA-02 600 cP At 25°C
Mix ratio with EA-028 100:28 parts by weight Resin : curing agent
Mixed viscosity with EA-028 500 cP At 25°C
Mix ratio with EA-87 100:37 parts by weight Resin : curing agent
Mixed viscosity with EA-87 250 cP At 25°C
Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Resin color Amber N/A As supplied
Resin specific gravity 1.13 N/A As supplied
Mix ratio with EA-02 100:11 parts by weight Resin : curing agent
Mixed viscosity with EA-02 600 cP At 25°C
Mix ratio with EA-028 100:28 parts by weight Resin : curing agent
Mixed viscosity with EA-028 500 cP At 25°C
Mix ratio with EA-87 100:37 parts by weight Resin : curing agent
Mixed viscosity with EA-87 250 cP At 25°C