CONAPOXY AD-1146

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

CONAPOXY AD-1146

Main features

  • Heat-Cured Polyurethane Adhesive Primer
  • 1,500 to 2,750 cP Viscosity Range
  • 0.5 to 1.5 MIL Dry-Film Target

Product Description

CONAP AD-1146 Adhesive Primer is a solvent-borne, heat-cured primer used to prepare supported substrates for bonding with liquid polyurethanes during cure. The primer can be applied by spray, roller coating, doctor blade, or brushing. Typical viscosity is 1,500-2,750 cP at 25 deg C, solids content is 23.0-25.0%, and thermal activation is used before polyurethane application. Documented applications include metal priming, glass and glass-fiber laminates, and wood and leather. Surface cleanliness, solvent removal, primer thickness, and thermal activation are central to the documented AD-1146 process.

Key features

  • Processing window: Solvent-borne, heat-cured primer for bonding liquid polyurethanes to supported substrates.
  • Flow and dispensing: Typical 1,500-2,750 cP viscosity at 25 deg C with 23.0-25.0% solids.
  • Key characteristic: Documented 0.5-1.5 mil dry-film target with 82-93 deg C activation for 1-2 hours.

Applications

  • Metal priming
  • Glass and glass-fiber laminates
  • Wood and leather

Technical Specifications

General Properties
Color
The color
Amber
Solids
23-25 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1500-2750 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
10 °C

Additional Information

Surface Treatments

Heat-activated primer for bonding liquid polyurethanes

CONAP AD-1146 is a solvent-borne, heat-cured primer used to prepare supported substrates for bonding with liquid polyurethanes during cure. The primer can be applied by spray, roller coating, doctor blade, or brushing. Typical viscosity is 1,500-2,750 cP at 25 deg C, solids content is 23.0-25.0%, and thermal activation is used before polyurethane application.

Solvent-borne primerHeat activated1,500-2,750 cP at 25 deg C23.0-25.0% solids0.5-1.5 mil dry film

As supplied

Typical material properties

The table is limited to the base CONAP AD-1146 primer and does not substitute values from AD-1146-C or AD-1146-C-1.

Property CONAP AD-1146 value Condition / method
Viscosity 1,500-2,750 cP 25 deg C / 77 F
Solids content 23.0-25.0% 1 g, 3 h, 105 deg C
Pounds per gallon 7.50 25 deg C / 77 F
Appearance Amber As supplied
Volatile organic content 5.7 lb/gal ASTM D3960
Flash point 10 deg C / 50 F ASTM D93

These are typical values and not specification limits.

Processing

Apply, dry, activate, then introduce the polyurethane

Surface cleanliness, solvent removal, primer thickness, and thermal activation are central to the documented AD-1146 process.

  1. Prepare surfaces so they are free of moisture, dirt, rust, chemicals, and mold release. Sandblasting, etching, or degreasing may be used as appropriate.
  2. Apply one or two coats of AD-1146 by soft brush, spray, roller coating, or doctor blade. Allow 30 minutes air dry between coats and at least 1 hour after the final coat.
  3. For spray application, one part AD-1146 may be diluted with up to two parts CONAP S-1 Solvent.
  4. Before applying polyurethane, activate the primer by baking at 82-93 deg C (180-200 F) for 1-2 hours.
  5. For optimum results, use a dry-film thickness of 0.5-1.5 mil; film thickness should not be below 0.5 mil.

Storage and handling

Store cool, dry, sealed, and out of direct sunlight

Store below 25 deg C (77 F) in a dry, controlled environment out of direct sunlight. Keep containers tightly sealed to minimize evaporation.

A 12-month suitability period from date of shipment applies when stored under the recommended conditions in original sealed containers. Mix the product thoroughly before use.

Technical guidance

Control cleanliness, residual solvent, and dry-film thickness

Bond quality depends on preparation of the actual substrate and complete solvent removal from the primer film.

Clean the substrate

Remove moisture, dirt, rust, chemicals, and mold release before applying the primer. Select sanding, etching, or degreasing for the actual substrate.

Remove residual solvent

Allow the specified air-dry periods. A 30-minute period at 70 deg C is identified for solvent evaporation from the primer film.

Control film thickness

Target 0.5-1.5 mil dry film and do not apply a dry film thinner than 0.5 mil.

Applications

Supported applications

Use the documented application scope below as the starting point for product evaluation.

Metal priming

Primer for supported metals including aluminum alloys, magnesium, iron, and steel before bonding with liquid polyurethanes.

Glass and glass-fiber laminates

Surface treatment for glass and glass-fiber laminate substrates before liquid-polyurethane bonding.

Wood and leather

Primer use on supported organic substrates such as wood and leather before liquid-polyurethane bonding.

Technical support for CONAP AD-1146 Adhesive Primer

Need help evaluating AD-1146 for a particular substrate, surface-preparation route, spray dilution, dry-film target, or heat-activation step? Krayden can help review the substrate condition, primer application method, drying sequence, activation temperature, and downstream polyurethane process before trials are run on the intended assembly.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers