CONAP DS-1831A

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONAP DS-1831A

Main features

  • 15% Red Pigment Concentrate
  • Epoxy and Polyurethane System Compatibility
  • Filled and Unfilled Formulation Guidance

Product Description

CONAP DS-1831A is a red color concentrate containing 15% pigment for compatible epoxy and polyurethane formulations used in electrical potting, casting, and encapsulation. Addition guidance varies for filled and unfilled resin systems and according to whether the concentrate is added to the base resin, curative, or total mixture. Documented applications include electrical potting, electrical casting, and electrical encapsulation. Keep the host formulation and point of addition together when selecting the applicable addition range.

Key features

  • Color control: 15% red pigment concentrate.
  • Material system: Epoxy and polyurethane system compatibility.
  • Key characteristic: Filled and unfilled formulation guidance.

Applications

  • Electrical potting
  • Electrical casting
  • Electrical encapsulation

Technical Specifications

General Properties
Color
The color
Red

Additional Information

Fine and specialty chemicals

CONAP DS-1831A red color concentrate

CONAP DS-1831A is the red grade within the CONAP DS-1830 Series of color concentrates for epoxy and polyurethane systems. It contains 15% pigment and is used to modify the color of compatible resin systems used for electrical potting, casting, and encapsulation.

The DS-1830 Series combines high compatibility with most epoxy and urethane systems with heat-stable pigments and improved heat and light resistance. DS-1831A may be incorporated into the appropriate resin component or into the total mixed system using the recommended addition ranges for filled and unfilled formulations.

Red concentrate 15% pigment Epoxy systems Polyurethane systems

Features and benefits

Color modification for epoxy and polyurethane formulations

Broad resin compatibility

The DS-1830 Series is highly compatible with most epoxy and urethane systems.

Heat-stable pigments

Heat-stable pigments support use in resin-system processing where color stability under heat is important.

Heat and light resistance

The series provides improved heat and light resistance for color modification of compatible formulations.

Product properties

DS-1831A identity and formulation role

DS-1831A is the 15% pigment red color concentrate within the CONAP DS-1830 Series.

Property State or scope Value
Product Product identity CONAP DS-1831A
Series Product identity CONAP DS-1830 Series
Color As supplied Red
Pigment concentration As supplied 15%
Compatible resin systems Formulation scope Epoxy and polyurethane systems
Primary application area Application Modification of resin systems used in electrical potting, casting, and encapsulation

Product selector

CONAP DS-1830 Series selector guide

Select the DS-1830 Series grade according to the required color and pigment concentration. DS-1831A is the red, 15% pigment grade shown on this page.

Product Color Pigment concentration Selection position
CONAP DS-1831A Red 15% Current product
CONAP DS-1832 Black 18% Black color concentrate
CONAP DS-1832 AP Black 18% Black color concentrate
CONAP DS-1833 Blue 50% Blue color concentrate
CONAP DS-1836 White 40% White color concentrate

Pigment concentration varies by grade. The amount of concentrate required in a formulation can also vary by color.

Formulation guidance

Choose the addition route for the resin system

The point of addition depends on whether the host formulation is an epoxy or polyurethane system. Mix the concentrate until all striations have disappeared and the material is homogeneous.

Epoxy systems

Mix the color concentrate with the epoxy Resin, Part A, or with the total mixed system.

Polyurethane systems

Mix the color concentrate with the polyurethane Curative, Part B, or with the total mixed system.

Host-system configuration Suggested concentrate addition Basis
Unfilled systems 3 to 5 parts by weight Per 100 parts by weight of base epoxy Resin or urethane Curative
Unfilled systems, total mixture basis 2% to 4% by weight Of the total mixed system
Filled systems 2 to 3 parts by weight Per 100 parts by weight of base epoxy Resin or urethane Curative

Adjustment guidance: The actual amount of color concentrate varies with the color used. Darker colors may require lower addition levels, while lighter colors may require higher amounts. Addition above the recommended levels may adversely affect the final properties of the cured epoxy or polyurethane system.

Application methods

Bench mixing for potting and casting formulations

Hand-mix bench processing

Suitable for hand-mix bench potting and casting operations.

Mechanical-mix bench processing

Suitable for mechanical-mix bench potting and casting operations.

Applications

Color modification for electrical protection materials

DS-1831A is used to modify compatible epoxy and polyurethane resin systems used in electrical potting, casting, and encapsulation.

Electrical potting

Adds red coloration to compatible resin systems used for electrical potting.

Electrical casting

Adds red coloration to compatible resin systems used for electrical casting.

Electrical encapsulation

Adds red coloration to compatible resin systems used for electrical encapsulation.

Regulatory information

RoHS compliance across the listed DS-1830 Series grades

CONAP DS-1831A, DS-1832, DS-1832 AP, DS-1833, and DS-1836 comply with Directive 2011/65/EU of the European Parliament and of the Council of 8 June 2011, RoHS 2.0, as amended 31 March 2015.

Products Compliance
DS-1831A, DS-1832, DS-1832 AP, DS-1833, DS-1836 RoHS 2.0, Directive 2011/65/EU as amended 31 March 2015

Storage and handling

Protect the concentrate from moisture and excessive temperature

Storage conditions

Store below 25°C / 77°F in a dry, controlled environment away from direct sunlight.

Shelf life

Shelf life is 12 months from the date of shipment when stored under the recommended conditions in the original sealed container.

Opened containers

The product is sensitive to moisture and atmospheric humidity. Once opened, use immediately or blanket the container with dry air or nitrogen before resealing.

Before use

Mix the product thoroughly before use.

Storage outside the recommended conditions may lead to deterioration in product performance.

Select the appropriate CONAP DS-1830 Series color concentrate

Krayden can help evaluate the appropriate DS-1830 Series grade and addition approach for the target epoxy or polyurethane formulation. Share the required color, resin chemistry, filled or unfilled formulation, batch size, mixing method, and potting, casting, or encapsulation process.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers