CHEMLOK 7701

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CHEMLOK 7701

Main features

  • Under Five-Minute Solvent Flash-Off
  • No-Mix Surface Conditioning
  • Wipe, Brush, Dip or Flood

Product Description

Chemlok 7701 Surface Treatment is a one-part, solvent-based surface treatment for preparing supported vulcanized and thermoplastic polymeric materials before bonding with compatible epoxy or urethane adhesives. It chemically alters the rubber surface to make it more receptive to downstream processing and must not be applied to metal surfaces. Chemlok 7701 requires no mixing and can be applied by wipe, brush, dip, or flood methods; spray application is not recommended. The treatment is complete after the solvent flashes off in less than five minutes, and no rinsing is required before subsequent bonding.

Key features

  • No-Mix Surface Treatment: supplied ready to use without component mixing
  • Fast Solvent Flash-Off: treatment is complete after solvent flash-off in less than five minutes
  • Flexible Manual Application: applies by wipe, brush, dip, or flood methods without a rinse step

Applications

Surface preparation of supported vulcanized and thermoplastic polymeric materials before bonding with compatible epoxy or urethane adhesives.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear to Cloudy Liquid
Density
Volumetric mass per unit
870-930 kg/m3
Solids
2.3-3.5 %
Solvent
Ethyl Acetate
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-4 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear to cloudy liquidTypical
Density870 to 930kg/m^3Typical
Solids by weight2.3 to 3.5%Typical
Flash point-4deg CSeta; typical
SolventEthyl acetateTypical
Solvent flash-offLess than 5minutesAfter application; no rinse required
Shelf life1yearOriginal unopened container; 21 to 27 deg C

Leading Brands Trust in Our Products and Services