CHEMLOK 607

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CHEMLOK 607

Main features

  • Clear One-Coat Silicone-Elastomer Bonding
  • Brush, Spray, or Dip Application
  • Extreme-Temperature Elastomer Bond Systems

Product Description

Chemlok® 607 Adhesive is a clear, one-coat adhesive for bonding unvulcanized silicone rubber and selected specialty elastomers to metal and nonmetal substrates. Documented substrate classes include metals, glass, plastics, textiles, and fabrics, while supported elastomers include silicone, fluoroelastomer, polyacrylate, epichlorohydrin, and selected peroxide-cured grades. The low-solids liquid may be applied by brush, spray, or dip after suitable surface preparation and dilution. Typical air-dry time is 10 to 30 minutes at room temperature before the coated part is bonded and the elastomer is cured.

Key features

  • One-coat elastomer bonding: The adhesive bonds unvulcanized silicone and selected specialty elastomers to diverse substrates.
  • Brush, spray, or dip application: The liquid may be diluted with methanol or ethanol for the selected coating method.
  • High- and low-temperature bonds: Bond systems with silicone or fluoroelastomers are documented above 204°C and below -51°C.

Applications / Suitable for

  • Bonding unvulcanized silicone rubber to metals, glass, plastics, and textiles
  • Bonding fluoroelastomer, polyacrylate, and epichlorohydrin compounds
  • Peroxide-cured silicone, nitrile, and hydrogenated-nitrile elastomer bonding

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear to Slightly Yellow Liquid
Density
Volumetric mass per unit
820 - 840 kg/m3
Solvent
Methanol, Ethanol
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
9 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Appearance Clear to slightly yellow liquid N/A As supplied
Density 820 to 840 kg/m³ As supplied
Solids content 6.2 to 6.8 % by weight Typical
Solvents Methanol and ethanol N/A As supplied
pH 8.5 to 10.5 N/A Typical
Air-dry time 10 to 30 min At room temperature
Optional heat drying 15 min At 104°C

Leading Brands Trust in Our Products and Services