CHEMLOK 485

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

CHEMLOK 485

Main features

  • One-Month Mixed Working Life
  • 17.8 to 25.4 um Film
  • Spray, Brush or Dip Application

Product Description

Chemlok 485 / Curative 44 Adhesive System is a two-component insert-molding adhesive system for bonding supported PVC and Alcryn-type thermoplastic elastomers to metal and rubber substrates. The system is prepared by adding 6 to 10 parts Curative 44 by weight to 100 parts Chemlok 485. When sealed from moisture at room temperature, the mixed material has an approximate working life of one month. It can be applied by spray, brush, or dip, with a recommended dry film thickness of 17.8 to 25.4 um before molding. The system is intended for supported insert-molding applications using the documented surface preparation and drying process.

Key features

  • Controlled Two-Component Mix: mix 100 parts Chemlok 485 with 6 to 10 parts Curative 44 by weight
  • Extended Mixed Working Life: mixed material has an approximate one-month working life at room temperature when sealed from moisture
  • Defined Dry Film: recommended dry film thickness is 17.8 to 25.4 um before molding

Applications

Insert molding of supported PVC and Alcryn-type thermoplastic elastomers to metal and rubber substrates.

Technical Specifications

Physical Properties
Viscosity (Part A)
400 -1000 mPa.s
Viscosity (Part B)
<10 mPa.s
General Properties
Density
Volumetric mass per unit
part A: 850.8 - 874.7/ Part B: 1010.0 -1040.0 kg/m3
Solvent
part A: MEK, Xylene/ part B: Xylene

Additional Information

Technical properties

As-supplied / before-processing properties

Component properties and mixed-system handling values are identified separately.

PropertyValueUnitMethod / condition
Chemlok 485 viscosity400 to 1000cps25 deg C; Brookfield LVT, spindle 2, 30 rpm; typical
Curative 44 viscosityLess than 10cps25 deg C; typical
Chemlok 485 density850.8 to 874.7kg/m^3Typical
Curative 44 density1010 to 1040kg/m^3Typical
Chemlok 485 solids by weight15 to 17%Typical
Curative 44 solids by weight47 to 51.5%Typical
Mix ratio100 : 6 to 10parts by weightChemlok 485 : Curative 44
Mixed working lifeApproximately 1monthRoom temperature; sealed from moisture