CG 1305

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CG 1305

Main features

  • Medium Density Syntactic
  • High-Strength Structural Bonding
  • Pourable Bonding Material

Product Description

Huntsman CG-1305 Resin/Hardener Epoxy Syntactic is a medium-density, pourable epoxy syntactic system developed for aircraft production and industrial applications that require a combination of high strength and low weight. The two-component system is designed for reinforcing high-stress areas in honeycomb structures and for potting applications. CG-1305 offers good handling characteristics, a density of 0.90 g/cc maximum when mixed, and extended working time with a gel time exceeding 60 minutes at 25°C. The material is qualified to BMS 5-28 Type 7 Class 1 and develops compressive strengths up to 9.0 ksi after elevated-temperature cure schedules, making it suitable for structural reinforcement and lightweight filling applications.

Key features

  • Medium-density syntactic epoxy: Combines low weight and structural strength for aerospace and industrial reinforcement applications.
  • Pourable processing characteristics: Mixed viscosity of approximately 21,500 cP and gel time greater than 60 minutes at 25°C support handling and placement.
  • BMS-qualified performance: Qualified to BMS 5-28 Type 7 Class 1 and capable of achieving compressive strengths up to 9.0 ksi after cure.

Applications / Suitable for

  • Reinforcing high-stress areas in honeycomb structures
  • Aircraft production assemblies
  • Potting applications
  • Lightweight structural filling applications

Technical Specifications

General Properties
Color
The color
Off-white
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Resin / Hardener)
Density (g)
0.90 max. g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Representative handling and processing properties of the mixed CG-1305 epoxy syntactic system.

Property Value Unit Method / condition
Color Off-white - Mixed material
Density 0.90 max. g/cc ASTM D792, mixed
Viscosity 21,500 cP 25°C, ASTM D2196
Gel Time >60 min 60 g mass at 25°C, ASTM D2471
Mix Ratio 100:20 wt. Resin : Hardener
Shelf Life 12 months Unopened containers at 25°C
Technical properties

After-processing / final-state properties

Typical cured-property data. Values are not intended as specifications.

Property Value Unit Method / condition
Compressive Strength 8.8 ksi ASTM D695, RT gel + 90 min @ 127°C
Compressive Modulus 420 ksi ASTM D695, RT gel + 90 min @ 127°C
Lap Shear Strength 1800 psi Al/Al, ASTM D1002, RT gel + 90 min @ 127°C
Weight Gain 0.50 % 24 h distilled water immersion, ASTM D543
Flammability Burn Rate 3 max. in./min 12-second vertical burn