BOSTIK NSBT-8N

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

BOSTIK NSBT-8N

Main features

  • Copper-Free Pure-Nickel Protection
  • Severe-Service Assembly Protection
  • Compact 8 oz Package

Product Description

Bostik Never-Seez Pure Nickel Special Anti-Seize Compound - 8 oz is a copper-free pure-nickel anti-seize compound supplied in an 8 oz can for threaded and fitted metal assemblies. The Pure Nickel Special grade provides anti-seize protection where a copper-free assembly lubricant is required and is approved for severe-temperature or aggressive service environments. Its paste form is applied at metal interfaces to support assembly and later disassembly while limiting seizure during service. The 8 oz configuration provides a smaller package option for supported maintenance and assembly work using the same Pure Nickel Special grade.

Key features

  • Copper-Free Pure-Nickel Grade: pure-nickel anti-seize chemistry supports applications where a copper-free assembly lubricant is required
  • Severe-Service Assembly Use: approved for supported threaded and fitted metal assemblies in severe-temperature or aggressive environments
  • Compact Package: 8 oz can supports smaller-volume assembly and maintenance requirements

Applications

Anti-seize protection of supported threaded and fitted metal assemblies in severe-temperature or aggressive environments.

Technical Specifications

General Properties
Color
The color
Silver Gray
Density (g)
1.24 - 1.3 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>250 °C
Operating Temperature
(-)183 to 1316 °C
Chemical Properties
Copper Corrosion
No Corrosion