BOSTIK L4145

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK L4145

Main features

  • One-Part No-Curative Nitrile Adhesive
  • Oil, Water, and Plasticizer Resistance
  • BMS 5-30/BAC5010 Qualification

Product Description

Bostik LIQ. 4145-30H is a one-part, solvent-based adhesive based on nitrile rubber for upholstery and interior trim bonding applications. The fast-drying, high-viscosity formulation produces a tough, elastic bond while providing resistance to oil, plasticizer migration, water, and detergents. It is designed for bonding vinyl, plastics, foam, metals, and fabrics used in automotive, rail, and aerospace interior assemblies, and meets Boeing BMS 5-30 Type I and BAC5010 Type 48 product specifications. :contentReference[oaicite:0]{index=0}

Key Features

  • One-part nitrile adhesive requires no separate curative, simplifying handling and processing.
  • Fast-drying, high-viscosity formulation develops a tough, elastic bond for upholstery and interior trim.
  • Resists oil, plasticizer migration, water, and detergents for durable interior assemblies.
  • Broad substrate compatibility with vinyl, plastics, foam, metals, fabrics, aluminum, ABS, and urethane materials.

Applications / Suitable For

  • Automotive interior trim
  • Rail interior trim
  • Aerospace interior trim and upholstery
  • Bonding vinyl to flexible and rigid plastics
  • Bonding foam, metals, fabrics, aluminum, ABS, and urethane materials

Technical Specifications

General Properties
Process Method
Solvent evaporation
Product Type
Material category or functional product class.
Solvent-based nitrile adhesive
Thermal Properties
Operating Temperature
N/A °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Product type One-part solvent-based nitrile adhesive — Supplier classification
Polymer base Nitrile — Typical physical property
Appearance Yellow-brown liquid — Typical physical property
Specific gravity 0.88 — Typical physical property
Total solids 30 % Typical physical property
Viscosity 8,000 cP Typical physical property
Solvent system Acetone, MEK — Supplier formulation
Flash point -23 °C Typical physical property
Shelf life Approximately 270 days — Stored at 13–49°C in sealed original container
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Bond type Tough, elastic bond — After solvent evaporation
Performance Resistant to oil, plasticizer migration, water and detergents — Supplier description
Application method Brush or roll coat — Clean, dry substrates
Alternative bonding process Allow first surface to dry ≥20 minutes; second surface bonded while tacky within 10 minutes — Supplier application procedure
Qualification Meets BMS 5-30 Type I and BAC5010 Type 48 — Supplier qualification