BOSTIK ISR70-03A

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK ISR70-03A

Main features

  • Primerless Elastic Silyl-Modified-Polymer Bonding
  • Solvent-, Isocyanate-, and PVC-Free Formulation
  • Transportation and Industrial Assembly Bonding

Product Description

Bostik ISR 70-03A is a one-component, moisture-curing adhesive and sealant based on Silyl Modified Polymer (SMP) technology. It is designed for elastic construction joints requiring high strength while providing excellent workability and durable long-term performance. The solvent-, isocyanate-, and PVC-free formulation offers primerless adhesion on many substrates, permanent elasticity, excellent UV and weather resistance, and compatibility with most industrial paint systems after skin formation. :contentReference[oaicite:0]{index=0}

Key Features

  • High-strength SMP adhesive and sealant for elastic construction joints.
  • Primerless adhesion to many common industrial substrates.
  • Permanent elasticity with excellent UV and weather resistance.
  • Low residual tack with fast moisture curing and excellent workability.

Applications / Suitable For

  • General bonding and sealing
  • Sunroof assemblies
  • Composite assembly
  • Bus, caravan, train and truck construction
  • Roof bonding
  • Bonding floor systems
  • Bonding aluminum or polyester corner profiles
  • Sealing welded seams

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
SMP adhesive & sealant
Thermal Properties
Operating Temperature
-40°C to +120°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Product type One-component Silyl Modified Polymer (SMP) adhesive and sealant — Moisture curing
Basic material Silyl Modified Polymer — Supplier classification
Curing method Moisture — Typical property
Specific gravity Approx. 1.4 g/mL Typical property
Skin-forming time 10 minutes 70°F (20°C), 50% RH
Open time <15 minutes 70°F (20°C), 50% RH
Curing speed after 24 hours 3 (0.125) mm (in.) Typical property
Green strength 300 Pa Physical Rheometer MC100
Application temperature 5 to 35 (40 to 95) °C (°F) Recommended application range
Shelf life 18 months (cartridges); 12 months (sausages) — Stored unopened at 5°C to 30°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness Approx. 55 Shore A Typical cured property
Volume change <3 % Typical cured property
Tensile stress (100%) 2.3 (245) MPa (psi) Typical cured property
Tensile stress at break 2.6 (275) MPa (psi) Typical cured property
Elongation at break 250 % Typical cured property
Lap shear strength 2.5 (360) MPa (psi) Typical cured property
E-Modulus (10%) 3.3 (475) MPa (psi) Typical cured property
Temperature resistance (continuous) -40 to 120 (-40 to 250) °C (°F) Typical cured property
Short-term temperature resistance 180 (350) °C (°F) Maximum 30 minutes
UV and weather resistance Excellent — Supplier classification