BOSTIK 940FS

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 940FS

Main features

  • 10-Minute Cure Cycle
  • Adhesion and Mechanical Performance of Polyurethane
  • Primerless Glass-to-Aluminum Bonding

Product Description

Bostik Marine 940 Fast Set Adhesive/Sealant is a one-component, rapidly moisture-curing adhesive and sealant based on Silyl Modified Polymer (SMP) technology. Designed for demanding marine environments, it combines the adhesion and mechanical performance of a polyurethane with the flexibility and UV resistance of a silicone. The solvent-free, isocyanate-free formulation provides permanent elastic bonding, excellent weatherability, fast skin formation, and strong primerless adhesion to many marine substrates for above- and below-the-waterline applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Fast-setting SMP adhesive with approximately 10-minute skin time and one-day cure for rapid assembly.
  • Primerless adhesion to aluminum, steel, fiberglass, EPDM rubber, PVC, glass, and painted surfaces in many applications.
  • Excellent UV and weather resistance with permanent elasticity from -40°C to 100°C.
  • Solvent-free and isocyanate-free formulation that is paintable after skin formation and sandable after full cure.

Applications / Suitable For

  • Marine bonding and sealing
  • Above- and below-the-waterline applications
  • Deck hardware installation
  • Through-hull fittings
  • Rub rails
  • Porthole sealing
  • Bonding aluminum, steel, fiberglass, EPDM rubber and PVC components

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
SMP marine adhesive/sealant
Thermal Properties
Operating Temperature
-40°C to +100°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Silyl Modified Polymer (SMP) — One-component moisture curing
Work life / Open time 15 minutes Typical uncured property
Skin time 10 minutes Typical uncured property
Curing time 1 day 77°F / 50% RH / 0.125 in. bead
Application temperature 40–95 (5–35) °F (°C) Recommended application range
Green strength 2.3 lb-force/ft² 0.125 in. thick, without sag
Shelf life 18 months (cartridges); 12 months (sausages) — Stored between 40°F and 80°F (5°C to 27°C)
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness 55 Shore A After 14 days at 77°F and 50% RH
Specific gravity 1.4 g/mL Typical cured property
Tensile strength @ 100% 400 psi Typical cured property
Tensile strength @ break 450 psi Typical cured property
Tensile shear strength 375 psi Aluminum-to-aluminum, 0.08 in. bondline
Elongation 225 % Typical cured property
Temperature resistance -40 to 212 (-40 to 100) °F (°C) Maintains elasticity in service
UV / Weather resistance Excellent — Supplier classification
Paintability After skin formation — Supplier recommendation
Sandability After full cure — Supplier recommendation