BOSTIK 9252

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BOSTIK 9252

Main features

  • Compatible Bostik Adhesive-System Priming
  • Aerospace-Specification Metal Priming
  • Brush-Applied Liquid Primer Format

Product Description

Bostik 9252 Primer is a thin, yellow-to-brown, brush-applied, solvent-based liquid primer for metal surfaces used ahead of bonding with compatible Bostik adhesive systems. It is referenced under DTD 900/4679A and AFS1179B aerospace specification listings. The primer is applied by brush to prepare supported metal surfaces, and it is intended for use with the specific Bostik adhesive system it supports rather than as a standalone bonding product.

Key features

  • Brush-Applied Metal Primer: thin, yellow-to-brown, brush-applied liquid for metal surface preparation
  • DTD 900/4679A and AFS1179B Reference: referenced under these aerospace specification listings
  • Compatible Bostik Adhesive-System Priming: applied ahead of bonding with compatible Bostik adhesive systems

Applications

Priming supported metal surfaces before bonding with compatible Bostik adhesives.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Thin Liquid
Color
The color
Yellow/Brown
Density (g)
1.0 g/cm3
Solids
30 %