BOSTIK 70-08A

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 70-08A

Main features

  • High-Green-Strength SMP Adhesive
  • Primerless Glass Bonding
  • Solvent-, Isocyanate-, and PVC-Free Formulation

Product Description

Bostik 70-08A is a one-component, moisture-curing adhesive based on Silyl Modified Polymer (SMP) technology, specifically developed for windscreen bonding and high-performance industrial assemblies. The high-green-strength formulation enables immediate or rapid movement of bonded components during manufacturing while providing durable, permanently elastic bonds. The solvent-, isocyanate-, and PVC-free adhesive offers primerless adhesion on many substrates, excellent UV and weather resistance, low electrical conductivity, and conforms to FMVSS 212 requirements for automotive glass glazing.

Key Features

  • High green strength enables immediate handling and transportation of bonded assemblies after installation.
  • Primerless adhesion to ceramic-coated automotive glass and many industrial substrates under supported conditions.
  • FMVSS 212 compliant for automotive glass glazing applications.
  • Permanent elasticity with excellent UV and weather resistance from -40°C to 120°C.

Applications / Suitable For

  • Automotive windscreen bonding
  • Glass glazing
  • Panel bonding
  • High-performance industrial assemblies
  • OEM manufacturing
  • Coachwork and mobile-unit assembly

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
SMP windscreen adhesive
Thermal Properties
Operating Temperature
-40°C to +120°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Basic material Silyl Modified Polymer (SMP) — Supplier classification
Curing method Moisture cure — One-component system
Specific gravity Approx. 1.4 g/mL Typical value
Skin-forming time 10 minutes Typical value
Open time <15 minutes Typical value
Curing speed after 24 hours 3 (0.125) mm (in.) Typical value
Green strength Approx. 1800 Pa Typical value
Application temperature 5–35 (41–95) °C (°F) Recommended application range
Solvent content 0 % Supplier value
Isocyanate content 0 % Supplier value
Shelf life 9–18 months depending on package size — Stored unopened at 5–30°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness Approx. 65 Shore A Typical cured property
Volume change <3 % Typical cured property
Tensile stress (100%) 2.1 (300) MPa (psi) Typical cured property
Tensile stress at break 2.9 (420) MPa (psi) Typical cured property
Elongation at break Approx. 225 % Typical cured property
Shear strength Approx. 2.5 (360) MPa (psi) Typical cured property
Tear propagation Approx. 13 N/mm Typical cured property
E-Modulus (10%) 4.3 (623) MPa (psi) Typical cured property
Temperature resistance -40 to 120 (-40 to 248) °C (°F) Continuous service
UV and weather resistance Very good — Supplier classification